Abstract
Thin hard coatings provide the much needed protection for steel thixoforming tools that must resist wear at high temperatures. The wear resistance of AlTiN- and AlTiON-coated hot work tool steel was investigated at 1023 K (750 °C), measured to be the cavity surface temperature shortly after the steel slurry was forced into the thixoforming die. The wear tests were repeated in exactly the same fashion with uncoated tool steel samples to identify the impact of AlTiN and AlTiON coatings on the high-temperature wear performance of X32CrMoV33 tool steel. The nature, the thickness, and the adherence of the oxide scales impact the tribological behavior. The poor adherence and limited ductility of ferrous oxides promote the failure of the oxide scale impairing the resistance to wear of the hot work tool steel at elevated temperatures. The substantial softening in the X32CrMoV33 hot work tool steel is also critical in the wear volume loss it suffers. AlTiN and AlTiON coatings, on the other hand, form a stable and protective oxide surface layer at high temperatures and therefore provide an enhanced resistance to oxidation. The latter is relatively more resistant to oxidation and is thus the better of the two coatings tested in the present work.
Similar content being viewed by others
References
S. Muenstermann, K. Uibel, T. Tonnesen, and R. Telle: Solid State Phenomena, 2006, vols. 116–117, pp. 696–99.
E. Lugscheider, K. Bobzin, C. Barimani, St. Barwulf, and T. Hornig: Adv. Eng. Mater., 2000, vol. 2, pp. 33–37.
Y. Birol: Mater. Sci. Eng., 2010, vol. A527, pp. 1938–45.
Y. Birol: Ironmaking and Steelmaking, 2010, vol. 37, pp. 41–46.
M.Z. Omar, E.J. Palmiere, A.A. Howe, H.V. Atkinson, and P. Kapranos: Mater. Sci. Eng., 2005, vol. A395, pp. 53–61.
E. Lugscheider, T. Hornig, D. Neuschutz, O. Kyrylov, and R. Prange: Proc. 6th Int. Conf. on Semi-Solid Processing of Alloys and Composites, Turin, 2000, G.L. Chiarmetta and M. Rosso, eds., Edimet-Spa, Torino, Italy, 2000, pp. 587–92.
R. Telle, S. Muenstermann, and C. Beyer: Solid State Phenomena, 2006, vols. 116–117, pp. 690–95.
Y. Birol: Steel Res. Int., 2009, vol. 80, pp. 165–71.
Y. Birol: Steel Res. Int., 2009, vol. 80, pp. 588–92.
Y. Birol: Ironmaking and Steelmaking, 2009, vol. 36, pp. 555–60.
A. Rassili, L. Adam, W. Legros, M. Robelet, D. Fischer, and A. Cucatto: Proc. 8th Int. Conf. on Semi-Solid Processing of Alloys and Composites (S2P), Limassol, Cyprus, Sept. 21–23, 2004, D. Apelian, A. Alexandrou, G. Georgiou, J. Jorstad, and M. Makhlouf, eds., University of Cyprus, Limassol, Cyprus, 2004.
P. Kapranos, D.H. Kirkwood, and C.M. Sellars: Proc. 4th Int. Conf. on Semi-Solid Processing of Alloys and Composites, H. Kirkwood and P. Kapranos, eds., The University of Sheffield, Sheffield, United Kingdom, 1996, pp. 306–11.
R. Kopp, E. Lugscheider, T. Hornig, J. Kallweit, M. Maes, and I. Seidl: Proc. 5th Int. ESAFORM Conf. on Material Forming, Akapit, Krakow, Poland, 2002, M. Pietrzyk, Z. Mitura, and J. Kaczmar, eds., Akapit, Krakow, Poland, 2002, p. 659.
P. Kapranos, D.H. Kirkwood, and C.M. Sellars: J. Eng. Manuf., 1993, vol. 207B, p. 1.
Y. Birol: Solid State Phenomena, 2008, vols. 141–143, pp. 289–94.
D.T. Peters, E.F. Brush, J.G. Cowie, and S.P. Midson: Die Casting toward the Future, North American Die Casting Association, Rosemont, IL, 2002, T02-065.
F.L. Riley: J. Am. Ceram. Soc., 2000, vol. 83, pp. 245–65.
Y. Birol: Ironmaking and Steelmaking, 2009, vol. 36, pp. 397–400.
Y. Birol: Ironmaking and Steelmaking, 2010, vol. 37, pp. 41–46.
Y. Birol: Int. J. Mater. Form., 2010, vol. 3, pp. 65–70.
O. Knotek, F. Löffler, and B. Bosserhoff: Surf. Coat. Technol., 1993, vol. 62, pp. 630–34.
A. Srivastava, V. Joshi, R. Shivpuri, R. Bhattacharya, and S. Dixit: Surf. Coat. Technol., 2003, vols. 163–164, pp. 631–36.
Y. Wang: Surf. Coat. Technol., 1997, vols. 94–95, pp. 60–63.
M. Rosso, D. Ugues, E. Torres, M. Perucca, and P. Kapranos: Int. J. Mater. Forming, 2008, vol. 1, pp. 1259–62.
L.A. Dobrzanski, M. Polok, and M. Adamiak: J. Mater. Process Technol., 2005, vols. 164–165, pp. 843–49.
E. Harry, M. Ignat, Y. Pauleau, A. Rouzaud, and P. Juliet: Surf. Coat. Technol., 2000, vol. 125, pp. 185–89.
L.S. Yul, K.G. Seong, and H.J. Hee: Surf. Coat. Technol., 2004, vols. 177–178, pp. 426–33.
T. Bjork, R. Westergard, S. Hogmark, J. Bergstrom, and P. Hedengvist: Wear, 1999, vols. 225–229, pp. 1123–30.
B. Navinsek, P. Panjan, I. Urankar, P. Cvahte, and F. Gorenjak: Surf. Coat. Technol., 2001, vols. 142–144, pp. 1148–54.
S.H. Ahn, J.H. Lee, J.G. Kim, and J.G. Han: Surf. Coat. Technol., 2004, vols. 177–178, pp. 638–44.
S.G. Harris, E.D. Doyle, A.C. Vlasveld, J. Audy, and D. Quick: Wear, 2003, vol. 254, pp. 723–34.
S. Paldey and S.C. Deevi: Mater. Sci. Eng., 2003, vol. A342, pp. 58–79.
S.Y. Lee and S.Y. Lee: Solid State Phenomena, 2006, vols. 116–117, pp. 84–87.
E. Lugscheider, K. Bobzin, T. Hornig, and M. Maes: Thin Solid Films, 2002, vols. 420–421, pp. 318–23.
K. Bobzin, N. Bagcivan, and P. Immich: Solid State Phenomena, 2008, vols. 141–143, pp. 249–54.
S.Y. Yoon, J.K. Kim, and K.H. Kim: Surf. Coat. Technol., 2002, vol. 161, pp. 237–42.
J.L. Mo and M.H. Zhu: Tribol. Int., 2009, vol. 42, pp. 1758–64.
M.H. Staia, M. D’Alessandria, D.T. Quinto, F. Roudet, and M. Marsal Astort: J. Phys.: Condens. Matter, 2006, vol. 18, pp. 1727–36.
R. Rodriguez-Baracaldo, J.A. Benito, E.S. Puchi-Cabrera, and M.H. Staia: Wear, 2007, vol. 262, pp. 380–89.
L.A. Dobrzanski, M. Polok, P. Panjan, S. Bugliosi, and M. Adamiak: J. Mater. Process. Technol., 2004, vols. 155–156, pp. 1995–2001
W.D. Munz: J. Vac. Sci. Technol., 1986, vol. A4, pp. 2717–25.
M. Kawate, A.K. Hashimoto, and T. Suzuki: Surf. Coat. Technol., 2003, vol. 165, pp. 163–67.
J.L. Endrino, G.S. Fox-Rabinovich, and C. Gey: Surf. Coat. Technol., 2006, vol. 200, pp. 6840–45.
G.S. Fox-Rabinovich, B.D. Beake, J.L. Endrino, S.C. Veldhuis, R. Parkinson, and L.S. Shuster: Surf. Coat. Technol., 2006, vol. 200, pp. 5738–42.
J. Sjolen, L. Karlsson, S. Braun, R. Murdey, A. Horling, and L. Hultman: Surf. Coat. Technol., 2007, vol. 201, pp. 6392–403.
M. Urgen, V. Ezirmik, E. Senel, Z. Kahraman, and K. Kazmanli: Surf. Coat. Technol., 2009, vol. 203, pp. 2272–77.
D. Isler, Y. Birol, and M. Urgen: Int. J. Mater. Form., 2010, vol. 3, pp. 747–50.
A. Knutsson: M.Sc. Thesis, Luleå University of Technology, Luleå, 2008.
O. Knotek and T. Leyendeckers: J. Solid State Chem., 1987, vol. 70, pp. 318–22.
Y. Birol and D. Isler: J. Non-Ferrous Met. Soc. China, 2010, vol. 20, pp. 1022–28.
M. Cornell and U. Schwertmann: The Iron Oxides, published online: Jan. 13, 2004, DOI:10.1002/3527602097.
S. Wilson and A.T. Alpas: Wear, 2000, vol. 245, pp. 223–29.
L. Rebouta, F. Vaz, M. Andritschky, and M.F. da Silva: Surf. Coat. Technol., 1995, vols. 76–77, pp. 70–74.
D. Mclntyre, J.E. Greene, G. Hakansson, J.E. Sundgren, and W.D. Munz: J. Appl. Phys., 1990, vol. 67, pp. 1542–53.
J.M. Challen and P.L.B. Oxley: Wear, 1979, vol. 53, pp. 229–43.
N.P. Suh and H.C. Sin: Wear, 1981, vol. 69, pp. 91–114.
K. Kutschej, P.H. Mayrhofer, M. Kathrein, P. Polcik, and C. Mitterer: Surf. Coat. Technol., 2005, vol. 200, pp. 1731–37.
S.-Y. Yoon, J.-K. Kim, and K.H. Kim: Surf. Coat. Technol., 2002, vol. 161, pp. 237–42.
R.J. Rodriguez, J.A. Garcia, A. Medrano, M. Rico, R. Sanchez, R. Matrinez, C. Lahaye, and A. Guette: Vacuum, 2002, vol. 67, pp. 559–66.
O. Barrau, C. Boher, R. Gras, and F. Rezai-Aria: Wear, 2007, vol. 263, pp. 160–68.
O. Joos, C. Boher, C. Vergne, C. Gaspard, T. Nylen, and F. Rezai-Aria: Wear, 2007, vol. 263, pp. 198–206.
A. Molinari, M. Pellizzari, A. Biggi, G. Corbo, and A. Tremea: Proc. 6th Int. Tooling Conf., Karlstadt University, Karlstadt, Sept. 2002, pp. 365–77.
D.J. Stephenson, J.R. Nicholls, and P. Hancock: Wear, 1986, vol. 111, pp. 15–29.
D.J. Stephenson, J.R. Nicholls, and P. Hancock: Wear, 1986, vol. 111, pp. 31–39.
Y. Birol: Wear, 2010, vol. 269, pp. 664–71.
L.H.S. Lung and T. Heijkoop: Wear, 1981, vol. 71, pp. 93–102.
P.A. Munther and J.G. Lenard: J. Mater. Proc. Technol., 1999, vol. 88, pp. 105–13.
T. Blazevic: Proc. 37th MWSP Conf., ISS-AIME, Warrendale, PA, 1996, vol. 33, pp. 33–38.
O. Barrau, C. Boher, R. Gras, and F. Rezai-Aria: Wear, 2003, vol. 255, pp. 1444–54.
Acknowledgments
F. Alageyik and O. Cakır are thanked for their help with the experiments. This work was funded by TUBITAK.
Author information
Authors and Affiliations
Corresponding author
Additional information
Manuscript submitted March 15, 2010.
Rights and permissions
About this article
Cite this article
Birol, Y., İsler, D. & Urgen, M. High-Temperature Sliding Wear Testing of Cathodic Arc Physical Vapor Deposition AlTiN- and AlTiON-Coated Hot Work Tool Steels. Metall Mater Trans A 42, 3316–3322 (2011). https://doi.org/10.1007/s11661-010-0474-1
Published:
Issue Date:
DOI: https://doi.org/10.1007/s11661-010-0474-1