Anodic oxide films grown on titanium alloy Ti-10V-2Fe-3Al in the solution of sodium tartrate, then sealed in boiling deionised water and calcium acetate solution were observed by using field emission scanning electron microscopy (FE-SEM), and were chemically analysed by using energy dispersive spectroscopy (EDS). Corrosion behaviour was investigated in a 3.5% sodium chloride solution, using electrochemical impedance spectroscopy (EIS). The morphology of the anodic oxide films was dependent on the sealing processes. The surface sealed in calcium acetate solution presented a more homogeneous and smooth structure compared with that sealed in boiling deionised water. The corrosion resistance of the oxide films sealed in calcium acetate solution was better than that sealed in boiling deionised water.

This is a preview of subscription content, log in via an institution to check access.

Access this article

Price excludes VAT (USA)
Tax calculation will be finalised during checkout.

Instant access to the full article PDF.

Similar content being viewed by others

References

  1. Hsu R W, Yang C C, Huang C A, et al. Electrochemical Corrosion Studies on Co-Cr-Mo Implant Alloy in Biological Solutions ACImpedance Measurements on Corroded Porous Aluminum Oxide Films[J]. Mater. Chem. Phys., 2005, 93: 531–538

    Article  Google Scholar 

  2. Pan J, Thierry D, Leygraf C. Hydrogen Peroxide Toward Enhanced Oxide Growth on Titanium in PBS Solution: Blue Coloration and Clinical Relevance[J]. J. Biomed. Mater. Res., 1996,30: 393–302

    Article  Google Scholar 

  3. Silva P L, Santos J D, Manterio F J, et al. Adhesion and Microstructural Characterization of Plasma-sprayed Hydroxyapatite/glass Ceramic Coatings onto Ti-6Al-4V Substrates AC-Impedance Measurements on Corroded Porous Aluminum Oxide Films[J]. Surf. Coat. Technol., 1998, 102: 191–196

    Article  Google Scholar 

  4. Yao Z P, Jiang Z H, Xin S G, et al. Electrochemical Impedance Spectroscopy of Ceramic Coatings on Ti–6Al–4V by Micro-plasma Oxidation[J]. Electrochimica Acta, 2005, 50: 3273–3279

    Article  Google Scholar 

  5. Souza M E P, Ballester M, Freire C M A. EIS Characterisation of Ti Anodic Oxide Porous Films Formed Using Modulated Potential[J]. Surf. Coat. Technol., 2007, 201: 7775–7780

    Article  Google Scholar 

  6. Liu J H, Yi J L, Li S M, et al. Influence of Electrolyte Concentration on the Morphology, Structure and Corrosion Resistance of Anodic Oxide Films on Ti-10V-2Fe-3Al Titanium Alloy[J]. J. Appl. Electrochem., 2010, 40: 1545–1553

    Article  Google Scholar 

  7. Wang B, Liu Z Q, Gao Y, et al. Microstructural Evolution During Aging of Ti-10V-2Fe-3Al Titanium Alloy[J]. J. Univ. Sci. Technol. Beijing, 2007, 4: 335–340

    Article  Google Scholar 

  8. Y Fovet, J Y Gal, A F T Chemla. Influence of pH and Fluoride Concentration on Titanium Passivating Layer Stability of Titanium Dioxide[J]. Talanta., 2001,53: 1053–1063

    Article  Google Scholar 

  9. Diamanti M V, Pedeferri M P, Effect of Anodic Oxidation Parameters on the Titanium Oxides Formation[J]. Corros. Sci., 2007, 49: 939–948

    Article  Google Scholar 

  10. Beranek R, Hildebrand H, Schmuki P. Self-organized Porous Titanium Oxide Prepared in H2SO4/HF Electrolytes[J]. Electrochim. Acta, 2005, 50: 3679–3684

    Article  Google Scholar 

  11. Bauer S, Kleber S, Schmuki P. TiO2 Nanotubes: Tailoring the Geometry in H3PO4/HF Electrolytes TiO2 Nanotubes: Tailoring the Geometry in H3PO4/HF Electrolytes[J]. Electrochem. Commun., 2006, 8: 1321–1325

    Article  Google Scholar 

  12. Yi J L, Liu J H, Li S M, et al. Morphology Evolution and Growth Mechanism of Porous Anodic Oxide Films on Titanium Alloy Ti-10V-2Fe-3Al in Neutral Tartrate Solution[J]. J. Cent. South Univ. Technol., 2011, 18(1): 6–15

    Article  Google Scholar 

  13. Gaponenko N V, Hluzd Y V, Maliarevich G K, et al. Room-temperature Photoluminescence From Porous Anodic Alumina Films with Wmbedded Terbium and Europium Species[J]. Mater. Lett., 2009, 63: 621–624

    Article  Google Scholar 

  14. Zhang J S, Zhao X H, Zuo Y, et al. The Bonding Strength and Corrosion Resistance of Aluminum Alloy by Anodizing Treatment in a Phosphoric Acid Modified Boric Acid/Sulfuric Acid Bath[J]. Surf. Coat. Technol., 2008, 202: 3149–3156

    Article  Google Scholar 

  15. Zuo Y, Zhao P H, Zhao J M. The Influences of Sealing Methods on Corrosion Behavior of Anodized Aluminum Alloys in NaCl Solution[J]. Surf. Coat. Technol., 2003, 166: 273–242

    Article  Google Scholar 

  16. HAO L, Cheng B R. Sealing Process of Anodic Coatings-past, Present, and Future[J]. Metal Finish, 2000, 12: 8–18

    Article  Google Scholar 

  17. Snogan F, Blanc C, Mankowski G, et al. Characterisation of Sealed Anodic Films on 7050 T74 and 2214 T6 Aluminium Alloys[J]. Surf. Coat. Technol., 2002, 154: 94–103

    Article  Google Scholar 

  18. Tamilselvi S, Raman V, Rajendram N. Corrosion Behaviour of Ti-6Al-7Nb and Ti-6Al-4V ELI Alloys in the Simulated Body Fluid Solution by Electrochemical Impedance Spectroscopy[J]. Electrochim. Acta, 2006, 52: 839–846

    Article  Google Scholar 

  19. Raman V, Tanmilselvi S, Rajendram N. Electrochemical Impedance Spectroscopic Characterization of Titanium During Alkali Treatment and Apatite Growth in Simulated Body Fluid[J]. Electrochim. Acta, 2007, 52: 7418–7424

    Article  Google Scholar 

  20. Kang M K, Moon S K, Lee S B, et al. Antibacterial Effects and Cytocompatibility of Titanium Anodized in Sodium Chloride, Calcium Acetate, and b-glycerol Phosphate Disodium Salt Pentahydrate Mixed Solution[J]. Thin Solid Films, 2009, 517: 5390–5393

    Article  Google Scholar 

  21. Hoar T P, Wood G C. The Sealing of Porous Anodic Oxide Films on Aluminium[J]. Electrochim. Acta, 1962,7: 333–353

    Article  Google Scholar 

  22. Hitzig J, Juettner K, Lorenz W J, et al. AC-Impedance Measurements on Corroded Porous Aluminum Oxide Films[J]. J. Electrochem.Soc., 1986, 133: 887–892

    Article  Google Scholar 

  23. Hitzig J, Juettner K, Lorenz W J, et al. AC-Impedance Measurements on Porous Aluminum Oxide Films[J]. Corros. Sci., 1984, 24: 945–952

    Article  Google Scholar 

  24. Laet J D, Scheers J, Terryn H, et al. Characterzation of Aluminium Surface Treatments with Electrochemical Impedance Spectroscopy and Spectroscopic Ellipsometry AC-Impedance Measurements on Corroded Porous Aluminum Oxide Films[J]. Electrochim. Acta, 1993, 38: 2103–2109

    Article  Google Scholar 

  25. Souza M E P, Ballester M, Freere C M A. EIS Characterisation of Ti Anodic Oxide Porous Films Formed Using Modulated Potential[J]. Surf. Coat. Technol., 2007, 201: 7775–7780

    Article  Google Scholar 

  26. Raman V, Nagarajan S, Rajendran N. Electrochemical Impedance Spectroscopic Characterization of Paßsive Film Formed over Ti-29Nb-13Ta-4.6Zf Alloy[J]. Electrochem. Commun., 2006, 8: 1309–1314

    Article  Google Scholar 

  27. Gonzalez J A, Lopez V, Bautista A, et al. Characterization of Porous Aluminium Oxide Films From AC Impedance measurements[J]. J. Appl. Electrochem., 1999, 29; 229–238

    Article  Google Scholar 

  28. Lizarbe R, Gonzalez J A, Lopez W, et al. Autosealing of Aluminuim Oxide Films[J]. Aluminium, 1992, 2: 140–144

    Google Scholar 

Download references

Author information

Authors and Affiliations

Authors

Corresponding author

Correspondence to Jianhua Liu  (刘建华).

Additional information

Supported by the National Natural Science Foundation of China (No.51271012)

Rights and permissions

Reprints and permissions

About this article

Check for updates. Verify currency and authenticity via CrossMark

Cite this article

Liu, J., Wu, L., Yu, M. et al. EIS characterization of sealed anodic oxide films on titanium alloy Ti-10V-2Fe-3Al. J. Wuhan Univ. Technol.-Mat. Sci. Edit. 31, 599–605 (2016). https://doi.org/10.1007/s11595-016-1416-6

Download citation

  • Received:

  • Accepted:

  • Published:

  • Issue Date:

  • DOI: https://doi.org/10.1007/s11595-016-1416-6

Key words

Navigation