Summary

Large pore MCM-41 was found to provide a better stabilization of Pd particles than amorphous SiO2 during liquid phase hydrogenation.  Pd/large pore MCM-41 exhibited higher hydrogenation activities as well as lower amount of metal loss by Pd leaching.

This is a preview of subscription content, log in via an institution to check access.

Access this article

Price excludes VAT (USA)
Tax calculation will be finalised during checkout.

Instant access to the full article PDF.

Similar content being viewed by others

Author information

Authors and Affiliations

Authors

Rights and permissions

Reprints and permissions

About this article

Cite this article

Panpranot, J., Pattamakomsan, K. & Praserthdam, P. Deactivation of silica supported Pd catalysts during liquid-phase hydrogenation. React Kinet Catal Lett 86, 141–147 (2005). https://doi.org/10.1007/s11144-005-0305-3

Download citation

  • Issue Date:

  • DOI: https://doi.org/10.1007/s11144-005-0305-3

Navigation