The effect of annealing temperatures on the resistance to delayed fracture and cyclic endurance of various regions of heat-affected zone of alloy OT4 is studied. Low-temperature maxima of resistance to delayed fracture and of cyclic endurance are discovered for the regions of heat-affected zone heated above the temperature of polymorphic transformation. The highest operating capacity under cyclic and long-term static loads is determined in the regions exposed to heating above 1000°C.
References
V. N. Moiseev, F. R. Kulikov, Yu. G. Kirillov, et al., Welded Joints of Titanium Alloys [in Russian], Metallurgiya, Moscow (1979).
B. A. Kolachev, V. A. Livanov, and A. A. Bukhanova, Mechanical Properties of Titanium and Its Alloys [in Russian], Metallurgiya, Moscow (1974).
I. I. Murav’ev, A. B. Kolomenskii, A. N. Roshchupkin, et al., “Effect of the temperature of vacuum annealing on the operating capacity of welded joints of titanium structures,” Svarochn. Proizvod., No. 11, 28 – 30 (1981).
M. N. Shushpanov, A. B. Kolomenskii, and A. N. Roshchupkin, “Special features of the process of fabrication of sheet welded structures from titanium alloys,” Svarochn. Proizvod., No. 3, 31 – 34 (2003).
Author information
Authors and Affiliations
Additional information
Translated from Metallovedenie i Termicheskaya Obrabotka Metallov, No. 4, pp. 39 – 41, April, 2009.
Rights and permissions
About this article
Cite this article
Shushpanov, M.N., Kolomenskii, B.A., Zubarev, V.Y. et al. Effect of annealing modes on the working capacity of the heat-affected zone of welds of alloy OT4. Met Sci Heat Treat 51, 191 (2009). https://doi.org/10.1007/s11041-009-9138-4
Published:
DOI: https://doi.org/10.1007/s11041-009-9138-4