The factorial experiment method is examined and a determination is made of the process parameters for electrocontact compaction (ECC) (time of application of pressure and electrical current, current density, and pressing pressure) that will ensure the production of a nearly pore-free material. A specific part is chosen for practical realization of the study results. The part passed tests performed under production conditions at the Institute of Thermoelectricity.
Similar content being viewed by others
References
Yu. G. Dorofeev, B. G. Gasanov, V. Yu. Dorofeev, et al., Commercial Technology for the Hot Pressing of Powder Products [in Russian], Metallurgiya, Moscow (1990).
S. N. Egorov, Yu. Yu. Medvedev, M. S. Egorov, et al., Russian Federation Patent No. 2210460, MKI B22F 3/105, Method of Making Products from a Charge Based on Metal Powder, submit. 12.06.2001. publ. 08.20.2003, Byul., No. 23.
S. N. Egorov, Yu. Yu. Medvedev, M. S. Egorov, et al., “Unit for the electrocontact compaction of metal powder,” Composite and Powder Materials. Structure, Properties, Technology: Symposium, Novocherkassk (2001), pp. 45–48.
S. N. Egorov and Yu. Yu. Medvedev, “Production of a high-density powder material by the method of electroplastic compaction,” Proc.: Modern Technologies in Materials Engineering, MGTU, Magnitogorsk (2003), pp. 99–102.
A. A. Spiridonov, The Use of Factorial Experiments in the Study of Production Processes [in Russian], Mashinostroenie, Moscow (1981).
Author information
Authors and Affiliations
Corresponding author
Additional information
Translated from Metallurg, No. 7, pp. 67–68, July, 2009.
Rights and permissions
About this article
Cite this article
Litvinova, T.A. Production of a high-density powder by electrocontact compaction. Metallurgist 53, 441 (2009). https://doi.org/10.1007/s11015-009-9204-6
Received:
Published:
DOI: https://doi.org/10.1007/s11015-009-9204-6