Abstract
The reliability of non-destructive evaluation depends on multitude of different factors. Consequently, it is difficult to assess the performance of the system. The only practical way to overcome this complexity and asses inspection reliability is using practical trials. In practical trials the inspection is performed on a known, flawed sample and reliability is judged by comparing the acquired inspection result with known state of the sample. However, confirming (and demonstrating), that the practical trials and, in particular, the used flaws are representative to postulated inspection case is, at present, challenging.
In this paper, the open literature is reviewed and compiled to the extent necessary for providing a starting point for confirming and demonstrating representativeness of flaws used in the practical trials. The available information on essential flaw parameters for various NDE techniques is reviewed. The used measurement methods for each parameter is discussed and the available in-service data summarized. Finally, a simple procedure is proposed for confirming and demonstrating the representativeness of used flaws.
Article PDF
Similar content being viewed by others
Avoid common mistakes on your manuscript.
References
Ahmed, S.R., Saka, M.: A sensitive ultrasonic approach to NDE of tightly closed small cracks. J. Press. Vessel Technol. 120, 384–392 (1998)
Becker, F.L., Doctor, S.R., Heasler, P.G., Morris, C.J., Pitman, S.G., Selby, G.P., Simonen, F.A.: Integration of NDE reliability and fracture mechanics—Phase I report. NUREG/CR-1696 PNL-3469, vol. 1, 170 p. (1981)
Crutzen, S.J., Jehenson, P., Nichols, R.W., McDonald, N.: The major results of the PISC II RRT. Nucl. Eng. Des. 115, 7–21 (1989)
Crutzen, S., Lemaitre, P., Iacono, I.: Realistic defects suitable for ISI capability evaluation and qualification. In: Proceedings of the 14th International Conference on NDE in the Nuclear and Pressure Vessel Industries, 24–26 September 1996, Stockholm, Sweden, pp. 153–163 (1996)
Denby, D., Duncumb, A.C.: The effects of stress on the ultrasonic detectability of defects. In: Proceedings of the Conference of Nondestructive Testing in the Fitness-for-Purpose Assessment of Welded Constructions, pp. 73–81. The Weldiung Institute, Cambridge (1984)
Edwards, R., Gruber, G., Watson, P.: Fabrication of performance demonstration initiative specimens with controlled flaws. In: Proceedings on 13th International Conference on NDE in the Nuclear and Pressure Vessel Industries, 22–25 May 1995, Kyoto, Japan, pp. 167–176 (1995)
Edwards, R.L., Watson, P.D., Gruber, G.J.: Fabrication of specimens with controlled flaws for procedure development and personnel training and qualification. In: Proceedings on 12th International Conference on NDE in the Nuclear and Pressure Vessel Industries, 11–13 October 1993, Philadelphia, Pennsylvania, USA (1993), pp. 93–100
Gauthier, V.: Thermal fatigue cracking of safety injection system pipes non destructive testing inspections feedback. In: Proceedings of NEA/CSNI Specialists’ Meeting on: Experiences with Thermal Fatigue in LWR Piping Caused by Mixing and Stratification, 8–10 June, Paris, France (1998), pp. 436–453
Green, E.R.: Worst-case defects affecting ultrasonic inspection reliability. Mater. Eval. 47, 1401–1407 (1989)
Ibrahim, S.I., Whittaker, V.N.: The influence of crack topography and compressive stresses on the ultrasonic detection of fatigue cracks in submerged arc welds. Br. J. NDT, September, pp. 233–240 (1981)
Iida, K., Takumi, K., Naruse, A.: Influence of stress condition on flaw detectability and sizing accuracy by ultrasonic inspection. In: The Ninth International Conference on Nondestructive Evaluation in the Nuclear Industry, 25–28 April, Tokyo, Japan, pp. 563–567 (1988)
Kemppainen, M., Virkkunen, I., Packalén, T., Sillanpää, J., Paussu, R.: Importance of crack opening in UT inspection qualification. In: Proceedings of the 6th International Conference on NDE in Relation to Structural Integrity for Nuclear and Pressurised Components, 8–19 October, Budapest, Hungary, p. 93–105 (2007)
Ogilvy, J.A.: Model for the ultrasonic inspection of rough defects. Ultrasonics 27, 69–79 (1989)
Packalén, T., Sillanpää, J., Kemppainen, M., Virkkunen, I., Paussu, R.: The influence of the crack opening in the UT inspection qualification. In: Proceedings of the 6th International Conference on NDE in Relation to Structural Integrity for Nuclear and Pressurised Components, 8–10 October, Budapest, Hungary, pp. 463–470 (2007)
Pirson, J., Roussel, G.: Emergency core cooling system pipe crack incident at the Tihange unit 1 plant. In: Proceedings of NEA/CSNI Specialists’ Meeting on: Experiences with Thermal Fatigue in LWR Piping Caused by Mixing and Stratification, 8–10 June, Paris, France, pp. 103–114 (1998)
Saka, M., Fukuda, Y.: NDT of closed cracks by ultrasonic propagation along the crack surface. NDT E Int. 24(4), 191–194 (1991)
Temple, J.A.G.: The effects of stress and crack morphology on time-of-flight diffraction signals. Int. J. Press. Vessels Piping 19, 185–211 (1985)
Toft, M.W.: Experimental studies of ultrasonic reflection from various types of misoriented defect. In: Proceedings of 21st Annual British Conference on Non-Destructive Testing – NDT, vol. 86, 193–206 (1986)
Waites, C., Whittle, J.: The status of performance demonstration and evaluation developments. Insight 40(12), 810–813 (1998)
Wirdelius, H., Osterberg, E.: Study of defect characteristics essential for NDT testing methods ET, UT and RT. SKI Project Number 98267, SKI Report 00:42, October 2000, Sweden, 50 p. (2000)
Wirdelius, H.: Probe model implementation in the null field approach to crack scattering. J. Nondestruct. Eval. 11(1), 29–39 (1992)
Wåle, J., Ekström, P.: Crack Characterisation for In-service Inspection Planning, SKI Projekt 14.4-940389, 94164 SAQ/FoU-Rapport 95/70, SAQ Kontroll AB, Stockholm, Sweden, 84 p. (1995)
Wåle, J.: Crack characterization for in-service inspection planning – an update. SKI reference 14.43-200543105, ISRN SKI-R-06/24-SE, SKI, Stockholm, Sweden (2006)
Yoneyama, H., Senoo, M., Miharada, H., Uesugi, N.: Comparison of echo heights between fatigue crack and EDM notch. In: Proceedings of 2nd International Conference on NDE in Relation to Structural Integrity for Nuclear and Pressurized Components, 24–26 May, 2000, New Orleans, Louisiana, USA, 8 p. (2000)
Author information
Authors and Affiliations
Corresponding author
Rights and permissions
Open Access This is an open access article distributed under the terms of the Creative Commons Attribution Noncommercial License (https://creativecommons.org/licenses/by-nc/2.0), which permits any noncommercial use, distribution, and reproduction in any medium, provided the original author(s) and source are credited.
About this article
Cite this article
Kemppainen, M., Virkkunen, I. Crack Characteristics and Their Importance to NDE. J Nondestruct Eval 30, 143–157 (2011). https://doi.org/10.1007/s10921-011-0102-z
Received:
Accepted:
Published:
Issue Date:
DOI: https://doi.org/10.1007/s10921-011-0102-z