The ultimate strength of boiler pipe metal made of martensitic chromium steel grade T91 is studied. Test results are close to European standard data. A dependence for calculating life characteristics of heat recovery boiler superheaters is obtained. It is shown that compared with domestic steel grade 10Kh9ÌFB of the same class T91 grade steel ultimate strength is higher. This discrepancy is related to the different nature of the steel structure.
Similar content being viewed by others
References
A. N. Tugov and M. N. Maidanik, “Steam boiler-utilizers for GTE with a capacity of more than 25 MW installed in Russian thermal power stations,” in: Proc. of Int. Sci.-Tech. Conf. “Problems of operating steam boiler-utilizers of steam and gas installations,” Moscow, 26 – 27 April (2018) [in Russian], OAO VTI, Moscow (2018).
V. A. Bogachev, “Residual life measuring device for convective and screen steam heaters,” Élektr. Stantsii, No. 6, 17 – 23 (2019).
SO 34.17.452-98. Procedural Instructions for the Order of Conducting Work During Evaluation of Electric Station Boiler Steam Heater Life [in Russian], VTI, Moscow (1998).
V. A. Bogachev and K. K. Kreiper, “Study of the ultimate strength of boiler pipe metal made of steel grade 10Kh9MFB (DI82),” Élektr. Stantsii, No. 8, 11 – 15 (2020).
V. A. Bogachev and O. V. Taran, “Effect of thermal non-equilibrium on temperature and reliability of convective steam heater metal,” Élektr. Stantsii, No. 2, 21 – 24 (2002).
EN 10216-2:2013. Seamless Steel Tubes for Pressure Purposes. Technical delivery conditions. Part 2. Non-Alloy and Alloy Steel Tubes with Specified Elevated Temperature Properties, European Standard, Brussels (2013).
Procedural Instructions for Determining Heat Resistance and Endurance Characteristics for Metal of Boilers, Pipes, and Pipelines [in Russian], TsPTI ORGRÉS, Moscow (2004).
STO 17230282.27.100.005–2008. Main Elements of Thermal Power Station Boilers, turbines, and Pipelines. Monitoring Metal Condition. Standards and Specifications [in Russian], OAO RAO EÉS Rossii, Moscow (2008).
Specimens for Testing Materials, Grips, and Transition Parts of Specimens. Normals N-82 [in Russian], VTI, Moscow (1982).
N. V. Bugai, T. G. Berezina, and I. I. Trunin, Power Generation Operating Capacity and Metal Endurance [in Russian], Énergoatomizdat, Moscow (1994).
GSSSD 141-89. Heat-Resistant Chromium Steel 10Kh9MFB (DI182-Sh). Nominal Yield Strength in the Temperature Range 500 – 610°C [in Russian], Izd. Standartov, Moscow (1990).
TU 14-3R-55-2001. Seamless Steel Pipes for Steam Boilers and Pipelines. Change No. 2 [in Russian], GNTs RF TsNIITMASh, Moscow (2001).
Author information
Authors and Affiliations
Corresponding author
Additional information
Translated from Élektricheskie Stantsii, No. 9, September 2021, pp. 29 – 33. DOI: 10.34831/EP.2021.23.28.005
Rights and permissions
Springer Nature or its licensor holds exclusive rights to this article under a publishing agreement with the author(s) or other rightsholder(s); author self-archiving of the accepted manuscript version of this article is solely governed by the terms of such publishing agreement and applicable law.
About this article
Cite this article
Bogachev, V.A., Kreitser, K.K. Study of the Ultimate Strength of Steel Grade X10CrMoVNb9-1 (T91) Boiler Pipe Metal. Power Technol Eng 55, 906–909 (2022). https://doi.org/10.1007/s10749-022-01451-2
Published:
Issue Date:
DOI: https://doi.org/10.1007/s10749-022-01451-2