Abstract
It is shown that the remaining life of bends of steam conduits from steel 15Kh1M1F should be evaluated on the basis of results of estimation of microdamage of the metal performed on a representative sample with allowance for the operating factors.
Similar content being viewed by others
References
RD 10-577-03. Type Instruction for Control of Metal and Prolonging the Service of Main Components of Boilers, Turbines, and Pipelines of Thermal Power Plants [in Russian], Moscow (2003).
V. A. Nakhalov, “Creep of a bent oval pipe loaded by internal pressure and bending moment,” Prikl. Mekh., No. 3 (1987).
V. A. Nakhalov, “Comparison of design evaluations of long-term strength and creep of bent and straight oval pipes from steel 12Kh1MF with experimental data,” Probl. Prochn., No. 8 (1990).
V. A. Nakhalov and Yu. V. Belomytsev, Reliability of Bends at Various Operating Parameters. Raising the Reliability and Evaluation of the Service Life of Bends of Unheated Boiler Pipes and Steam Conduits [in Russian], Chelyabinsk (1981).
RD 10-249-98. Norms of Strength Design of Stationary Boilers and Pipelines for Steam and Hot Water [in Russian].
G. M. Novitskaya and A. A. Rychkov, “Effect of cyclic changes in temperature and stress on the refractoriness of steel 15Kh1M1F,” Fiz. Met. Metalloved., 47(3) (1979).
Yu. V. Balashov and G. M. Novitskaya, “Evaluation of the endurance of parts of power equipment under variable operating conditions,” Probl. Prochn., No. 7 (1982).
Author information
Authors and Affiliations
Additional information
__________
Translated from Élektricheskie Stantsii, No. 3, March 2006, pp. 29–32.
Rights and permissions
About this article
Cite this article
Balashov, Y.V., Aznabaev, A.A., Slobodchikova, N.I. et al. Assessing the remaining life of bends of live steam conduits from steel 15Kh1M1F. Power Technol Eng 40, 175–178 (2006). https://doi.org/10.1007/s10749-006-0043-3
Issue Date:
DOI: https://doi.org/10.1007/s10749-006-0043-3