The following suspension composition is recommended for fabricating yarn by the hydrodynamic method: 3 g/liter methylcellulose; 2 g/liter Laprol 5003; 2 g/liter aluminum oxide fibre. It is useful to remix the suspension directly during use, providing the corresponding technical agents for realizing this condition in the yarn manufacturing setup.

This is a preview of subscription content, log in via an institution to check access.

Access this article

Price excludes VAT (USA)
Tax calculation will be finalised during checkout.

Instant access to the full article PDF.

Similar content being viewed by others

References

  1. A. V. Ageev and V. A. Volkov, Surface Phenomena and Disperse System in Production of Textile Materials and Chemical Fibres [in Russian], A. N. Kosygin MGTU, Sov’yazh Bevo Group, Moscow (2004).

  2. V. B. Tikhomirov, Design and Analysis of Experiments [in Russian], Legkaya INdustriya, Moscow (1974).

    Google Scholar 

Download references

Author information

Authors and Affiliations

Authors

Additional information

Translated from Khimicheskie Volokna, No. 5, pp. 31-33, September-October, 2009.

Rights and permissions

Reprints and permissions

About this article

Cite this article

Papilin, N.M., Kapitanov, A.F., Volkov, V.A. et al. Basis for the formula for the fibre suspension. Fibre Chem 41, 314–316 (2009). https://doi.org/10.1007/s10692-010-9195-x

Download citation

  • Published:

  • Issue Date:

  • DOI: https://doi.org/10.1007/s10692-010-9195-x

Keywords

Navigation