Abstract
The danger of the appearance of fibre segments of increased linear density over the ends of cylindrical packs in winding of mineral fibres was substantiated. Dependences were obtained that allow determining the helix angle of the loops at which the linear density of the fibre will not exceed the acceptable values when the direction of movement changes.
Similar content being viewed by others
References
A. F. Proshkov, Fibre Spreading Mechanisms (Design Questions) [in Russian], Legprombytizdat, Moscow (1986), p. 248.
L. I. Koroteeva, A. V. Sharonov, and A. P. Yaskin, Khim. Volokna, No. 1, 29–30 (2006).
V. I. Kostikov and L. N. Smirnov, Basalt Fibre Materials [in Russian], Informkonversiya, Moscow (2001), p. 158.
Author information
Authors and Affiliations
Additional information
__________
Translated from Khimicheskie Volokna, No. 6, pp. 44–45, November–December, 2007.
Rights and permissions
About this article
Cite this article
Koroteeva, L.I., Voronina, E.N. Features of formation of cylindrical packs of mineral fibres. Fibre Chem 39, 480–482 (2007). https://doi.org/10.1007/s10692-007-0105-9
Issue Date:
DOI: https://doi.org/10.1007/s10692-007-0105-9