The hygroscopicity of poly-α-olefin based oils is studied. Moisture saturation of all oils used in this study is reached by 60 h into the tests. The dependence of the hygroscopocity of the oils on the molecular mass of the oligomer is determined. The presence of functional additives in the oils does not greatly affect their hygroscopicity, while polar compounds (products of aging) sharply (almost twofold) increase the hygroscopicity.
Similar content being viewed by others
References
R. A. Lipshtein and M. N. Shakhnovich, Transformer Oil [in Russian], Énergiya, Moscow (1968), pp. 182–193.
A. I. Yechan, G. T. Novosartov et al., Neftepereerabotka Neftekhimiya, No. 2, 25–26 (1980).
A. I. Yechin, G. T. Novosartov, and E. A. Popova, Khim. Tekhnol. Topliv Masel, No. 4, 26–28 (1981).
G. D. Golovan’, T. B. Zhilyaev, A. I. Panchenko et al., Khim. Tekhnol. Topliv Masel, No. 8, 18–20 (1984).
Author information
Authors and Affiliations
Additional information
Translated from Khimiya i Tekhnologiya Topliv i Masel, No.4, pp. 24 – 26, July – August, 2011.
Rights and permissions
About this article
Cite this article
Naumova, T.I., Tyshchenko, V.A., Surovskaya, G.V. et al. Hygroscopicity of poly-α-olefin based oils. Chem Technol Fuels Oils 47, 278–282 (2011). https://doi.org/10.1007/s10553-011-0296-x
Published:
Issue Date: