It is shown that the initial state of uranium dioxide powder has no effect on the density, microstructure, and strength of pellets. Pore-forming agents and U3O8 used in fabrication lower the pellet strength because their particles are not spherical. To increase pellet strength, it is recommended that U3O8 be subjected to special processing to spheroidize the particles before mixing for uranium dioxide powder.

This is a preview of subscription content, log in via an institution to check access.

Access this article

Price excludes VAT (USA)
Tax calculation will be finalised during checkout.

Instant access to the full article PDF.

Similar content being viewed by others

References

  1. V. V. Gorskii, “Improvement of the uranium fuel for light-water reactors,” At. Tekh. Rubezh., No. 5, 3–12 (2000).

  2. I. S. Golovin and V. V. Novikov, “Serviceability of fuel elements with a change of power of thermal power reactors,” ibid., No. 3, 1–13 (1984).

  3. K. Radford and J. Pope, “UO2 fuel pellet microstructure modification through impurity additions,” J. Nucl. Mater., 116, No. 2, 305–313 (1983).

    Article  ADS  Google Scholar 

  4. H. Assman, W. Dörr, and M. Peehs, “Control of UO2 microstructure by oxidative sintering,” ibid., 140, No. 1, 1–6 (1986).

    Article  ADS  Google Scholar 

  5. K. Radford, “Effect of fabrication parameters and microstructure on the mechanical strength of UO2 fuel pellets,” ibid., 84, 222–236 (1979).

    Article  ADS  Google Scholar 

  6. V. V. Basov, A. V. Ivanov, V. S. Kurskov, et al., RF Patent No. 2148279 of April 27, 2000, “Method of obtaining fuel pellets,” Byull. Izobr. Polez. Modeli, No. 10, 273 (2000).

  7. OST 95 820–2006, Uranium Oxides: Polarographic Method for Measuring the Oxygen Ratio, VNIINM (2006).

  8. OI 001.387-97, Determination of the Density and Volume Fraction of Open and Closed Pores in Fuel Pellets by Hydrostatic Weighing With and Without Water Penetration into the Pores. Instruction, VNIINM (1997).

  9. 533.181.000 MVI, Parameters of the Microstructure of Uranium Dioxide Fuel Pellets. Measurement Procedure, VNIINM (1998).

Download references

Author information

Authors and Affiliations

Authors

Additional information

Translated from Atomnaya Énergiya, Vol. 107, No. 2, pp. 69–71, August, 2009.

Rights and permissions

Reprints and permissions

About this article

Cite this article

Petrov, I.V., Basov, V.V. Investigation of the influence of the initial state of powder, pore-forming additions, and U3O8 on the microstructure and strength of fuel pellets. At Energy 107, 85–88 (2009). https://doi.org/10.1007/s10512-009-9200-8

Download citation

  • Received:

  • Published:

  • Issue Date:

  • DOI: https://doi.org/10.1007/s10512-009-9200-8

Keywords

Navigation