Abstract
Linear wood welding of grooved surfaces to ease the elimination of water vapour and to increase the welding surface was performed in this study.
Similar content being viewed by others
References
Ganne-Chedeville C, Leban J-M, Properzi M, Pichelin F, Pizzi A (2006a) Temperature and density distribution in mechanical vibration wood welding. Wood Sci Technol 40:72–76
Ganne-Chedeville C, Properzi M, Pizzi A, Leban J-M, Pichelin F (2006b) Parameters of wood welding: a study with infrared thermography. Holzforschung 60:434–438
Gfeller B, Zanetti M, Properzi M, Pizzi A, Pichelin F, Lehmann M, Delmotte L (2003) Wood bonding by vibrational welding. J Adhes Sci Technol 17:1425–1590
European Norm EN 302-1 (2004) Adhesives for load-bearing timber structures
Omrani P, Mansouri HR, Pizzi A (2009) Emission gasses in linear vibration welding of wood. J Adhes Sci Technol 23:85–94
Omrani P, Masson E, Pizzi A, Mansouri HR (2008) Emission gases and degradation volatiles from polymeric wood constituents in wood dowels friction welding. Polym Degrad Stabil 93:794–799
Author information
Authors and Affiliations
Corresponding author
Rights and permissions
About this article
Cite this article
Omrani, P., Mansouri, H.R. & Pizzi, A. Linear welding of grooved wood surfaces . Eur. J. Wood Prod. 67, 479–481 (2009). https://doi.org/10.1007/s00107-009-0334-0
Received:
Published:
Issue Date:
DOI: https://doi.org/10.1007/s00107-009-0334-0