Skip to main content

Bentonite binder effective strength (BESt) test for unfired iron ore pellets

Abstract

Iron ore pellets use bentonite clay as binder at dosages of from 0.5% to 1.0% of the moist iron ore concentrate weight. As a natural product, bentonite has variable water-absorption and binding properties depending on its source. Therefore, it is best to have a method for evaluating a given bentonite to determine how effective it would be before it is purchased for use to bind concentrate into pellets. Current tests of bentonite effectiveness include plate water absorption (PWA), methylene blue uptake, free swell, exchangeable cations and glycolated layer expansion. However, these tests have many disadvantages. First, they only measure the ability of a bentonite to expand, disperse or absorb, and they do not directly measure how well it will bond particles to form iron ore pellets. Second, most of the tests require up to 20 hours to perform. Bentonite only has a few minutes to interact within the concentrate before it is indurated (sintered). For this reason, these long-term tests may not reflect the true behavior of bentonite during iron ore pelletization. Third, the tests are tedious and the results are often inconsistent for different iron ore concentrates, laboratories and technicians. Fourth, some of the testing equipment is difficult to procure. Fifth, procedures are often difficult to standardize. In this paper, the binder effectiveness strength (BESt) test to evaluate binders for iron ore pellets is presented. This procedure directly measures the ability of bentonite to form interparticle bonds, requires only about two hours to complete, is simple and reproducible, and it uses readily available equipment that has been standardized for decades. In this paper, results are given that demonstrate that the BESt results correlate well with actual pelletization performance.

This is a preview of subscription content, access via your institution.

References

  • American Foundrymen’s Society, 1978, Mold and Core Test Handbook, Des Plains, Illinois, Section 7, pp. 1–32

    Google Scholar 

  • ASTM E382-97, 1998, “Standard test method for determination of the crushing strength of iron ore pellets,” 1996 Book of ASTM Standards, Vol. 3.06, pp. 57–58, (Metals Test Methods and Analytical Procedures).

    Google Scholar 

  • ASTM E946-92, 1996, “Standard test method for water absorption of bentonite by the porous plate method,” Annual Book of ASTM Standards,” Vol. 3.06, pp. 276–277, (Metals Test Methods and Analytical Procedures).

    Google Scholar 

  • Dixon, W.J., and Massey, F.J., 1983, Introduction to Statistical Analysis, 4th Edition, McGraw-Hill, New York, pp. 83–84 and Table A5.

    MATH  Google Scholar 

  • Kawatra, S.K., and Ripke, S.J., 2001, “Developing and understanding the bentonite fiber bonding mechanism,” Minerals Engineering, Elsevier Science Ltd., Vol. 14, No. 6, p. 651

    Article  Google Scholar 

  • Kawatra, S.K., and Ripke, S.J., 2002, “Studies on the relationship between plate water absorption and iron ore pellet strength,” Minerals and Metallurgical Processing, Society for Mining, Metallurgy, and Exploration, Inc., Littleton, Colorado, Submitted May 2002, 11 pp.

    Google Scholar 

  • Ripke, S.J., and Kawatra, S.K., 2000, “Can fly-ash extend bentonite binder for iron ore agglomeration?” International Journal of Mineral Processing, December, Vol. 60, p. 187.

    Article  Google Scholar 

  • Ripke, S.J., and Kawatra, S.K., 2002, “Effect of cations on iron ore pellet strength,” Preprint 02-017, presented at the 2002 SME Annual Meeting, Phoenix, Arizona, 12 pp.

    Google Scholar 

Download references

Author information

Authors and Affiliations

Authors

Rights and permissions

Reprints and Permissions

About this article

Cite this article

Ripke, S.J., Kawatra, S.K. Bentonite binder effective strength (BESt) test for unfired iron ore pellets. Mining, Metallurgy & Exploration 21, 65–70 (2004). https://doi.org/10.1007/BF03403305

Download citation

  • Received:

  • Accepted:

  • Published:

  • Issue Date:

  • DOI: https://doi.org/10.1007/BF03403305

Key words

  • Bentonite binder
  • Pelletization
  • Strength test
  • Taconite processing