Cobalt pressure leaching and reduction at garfield

  • Technical Article
  • Published:
JOM Aims and scope Submit manuscript

Abstract

Cobalt recovery from arsenical concentrates by pressure leaching and reduction involves special methods and operating problems. Principal steps in the process are auto-oxidation acid leaching under pressure, filtration of the tailings, purification of the solution, hydrogen reduction of the ammoniacal solution, and melting in an electric arc furnace to remove sulfur and granulate the metal.

This is a preview of subscription content, log in via an institution to check access.

Access this article

Price excludes VAT (USA)
Tax calculation will be finalised during checkout.

Instant access to the full article PDF.

Similar content being viewed by others

Author information

Authors and Affiliations

Authors

Rights and permissions

Reprints and permissions

About this article

Check for updates. Verify currency and authenticity via CrossMark

Cite this article

Mitchell, J.S. Cobalt pressure leaching and reduction at garfield. JOM 9, 343–345 (1957). https://doi.org/10.1007/BF03398496

Download citation

  • Published:

  • Issue Date:

  • DOI: https://doi.org/10.1007/BF03398496

Navigation