Magnetic fields of flaw groups have been calculated with due account of flaw interaction. The density of magnetic charges induced on surfaces of flaws behind the first flaw of the group (in the direction of magnetizing field) is lower. Parameters charaterizing resolution of flaws in a group based on the magnetic field configuration have been determined.
Similar content being viewed by others
References
Clive, R., David, H.,et al., Nondestructive Testing of Operating Pipelines for Detection of Corrosion and Fatigue Cracks,4 Mezhdunarodnaya delovaya vstrecha Diagnostika 94 (4th International Business Meeting Diagnostics 94) (Yalta, 1994, pp. 44–60.
Barbian, O.A., New Developments in the Inside Inspection of Pipelines: Detection of Cracks,4 Mezhdunarodnaya delovaya vstrecha Diagnostika 94 (4th International Business Meeting Diagnostics 94), Yalta, 1994, pp. 149–159.
Gordon, A.M., On Configuration of Magnetic Fields Due to Localized Flaws,Defektoskopiya, 1976, no. 3, pp. 109–111.
Novikov, M.K., Shcherbinin, V.E., and Filippov, B.A., Magnetic Fields Generated by Flaws Slanted with Respect to the Workpiece Surface and Clusters of Flaws,Defektoskopiya, 1980, no. 3, pp. 106–108.
Bronshtein, N.N. and Semendyaev, K.A.,Spravochnik po matematike dlya inzhenerov i uchashchikhasya vtuzov (Reference Book on Mathematics for Engineers and Students of Technical Universities), Moscow: Nauka, 1986.
Author information
Authors and Affiliations
Rights and permissions
About this article
Cite this article
Zagidulin, R.V., Muzhitskii, V.F. & Kurozaev, V.P. Resolution of discontinuity flaws based on measurements of magnetic field configuration. Russ J Nondestruct Test 36, 344–352 (2000). https://doi.org/10.1007/BF02759418
Received:
Issue Date:
DOI: https://doi.org/10.1007/BF02759418