Abstract
The atomic force microscope (AFM) was used to monitor changes in surface features of an acrylic melamine coating that was exposed to a variety of conditions. Exposure to ultraviolet (UV) radiation and high relative humidity caused general roughening of the surface and the formation of pits. Further, the damage of the coating surface was much more substantial for exposure to high relative humidity compared to exposure to dry environments. This difference in degradation rates correlated with measurements of chemical degradation determined using infrared spectra that were acquired along with the AFM images.
Similar content being viewed by others
References
Climate Research Committee,Natural Climate Variability on Decade-to-Century Time Scales, National Academy of Science Press, Washington, DC, 1995.
Martin, J.W., “A Critical Review of the Role of Field Exposure Experiments in Predicting the Service Life of Coatings,”Durability of Coatings on Plastics, Ryntz, R.A. (Ed.), Hanser, New York, 2000.
Martin, J.W., Nguyen, T., Byrd, E., Dickens, B., and Embree, E., “Relating Laboratory and Outdoor Exposures of Acrylic Melamine Coatings: I. Estimation of Total Absorbed Dosage and Spectral Quantum Yield,”Poly. Degrad. Stab., submitted for publication, 2000.
Bauer, D.R., “Melamine/Formaldehyde Crosslinkers: Characterization, Network Formation and Crosslnk Degradation,”Prog. Org. Coat., 14, No. 3, 193 (1986).
Bauer, D.R., Gerlock, J.L., and Mielewski, D.F., “Photostabilization and Photodegradation in Organic Coatings Containing a Hindered Amine Light Stabilizer. 7. HALS Effectiveness in Acrylic Melamine Coatings Having Different Free-Radical Formation Rates,”Poly. Degrad. Stab., 36, No. 1, 9 (1992).
Bauer, D.R. and Mielewski, D.F., “The Role of Humidity in the Photooxidation of Acrylic Melamine Coatings,”Poly. Degrad. Stab., 40, No. 3, 349 (1993).
Hill, L.W., “Overview of Mechanical Property Changes During Coating Degradation,”Service Life Prediction of Organic Coatings: A Systems Approach, ACS Symposium Series 722, Bauer, D.R. and Martin, J.W. (Eds.), American Chemical Society, Washington, DC, pp. 312–322, 1999.
Hill, L.W., Korzeniowski, H.M., Ojunga-Andrew, M., and Wilson, R.C., “Accelerated Clearcoat Weathering Studies by Dynamic-Mechanical Analysis,” Prog. Org. Coat., 24, No. 1–4, 147 (1994).
Nichols M.E., Gerlock J.L., and Smith C.A., “Rates of Photooxidation Induced Crosslinking and Chain Scission in Thermoset Polymer Coatings,”Poly. Degrad. Stab., 56, No. 1, 81 (1997).
Nichols M.E., Darr C.A., Smith C.A., Thouless, M.D., and Fischer, E.R., “Fracture Energy of Automotive Clearcoats — I. Experimental Methods and Mechanics,”Poly. Degrad. Stab., 60, No. 2–3, 291 (1998).
Lee, F., Pourdeyhimi, B., and Adamsons, K., “Analysis of Coatings Appearance and Surface Defects Using Digital Image Capture-Processing-Analysis System,”Service Life Prediction of Organic Coatings: A Systems Approach, ACS Symposium Series 722, Bauer, D.R. and Martin, J.W. (Eds.), American Chemical Society, Washington, DC, pp. 207–232, 1999.
Klein, W.H. and Goldberg, B., “Monitoring UVB Spectral Irradiances at Three Latitudes,”Proc. International Solar Energy Society Conference (Vol. 1), 400 (1978).
Prane, J.A., “Introduction to Polymers and Resins,”Federation Series on Coatings Technology, Federation of Societies for Coatings Technology, Philadelphia, PA, 1986.
Rancourt, J.D.,Optical Thin Films User’s Handbook, McGraw-Hill, New York, p. 183, 1987.
Nguyen, T., Martin, J.W., Byrd, E., and Embree, N., “Effects of Relative Humidity on Photodegradation of Acrylic Melamine Coatings: A Quantitative Study,”Proc. American Chemical Society Division of Polymeric Materials: Science and Engineering, American Chemical Society, Washington, DC, 83, 188 (2000).
Martin, J.W., Nguyen, T., Byrd, E., Dickens, B., and Embree, E., “Relating Laboratory and Outdoor Exposures of Acrylic Melamine Coatings: II. Effects of Relative Humidity on Photodegradation, Absorbed Dosage and Apparent Quantum Yields of Acrylic-Melamine Coatings,”Journal of Coatings Technology, submitted for publication, 2001.
Gregorovich, B.V. and Hazan, I., “Environmental Etch Performance, and Scratch and Mar of Automotive Clearcoats,”Prog. Org. Coat., 24, No. 1–4, 131 (1994).
Holoubka, J.W., Schmitz P.J., and Xu, L.-F., “Acid Etch Resistance of Automotive Clearcoats. I: Laboratory Test Method Development,”Journal of Coatings Technology, 72, No. 901, 77 (2000).
Schmitz, P.J., Holoubka, J.W., and Xu, L.-F., “Mechanism for Environmental Etch of Acrylic Melamine-Based Automotive Clearcoats: Identification of Degradation Products,”Journal of Coatings Technology, 72, No. 904, 39 (2000).
Bauer, D. R., “Degradation of Organic Coatings. I. Hydrolysis of Melamine Formaldehyde/Acrylic Copolymer Films,”J. Appl. Polym. Sci., 27, No. 10, 3651 (1982).
Nichols, M.E. and Darr, C.A., “The Effect of Weathering on the Stress Distribution and Mechanical Performance of Automotive Paint Systems,”Service Life Prediction of Organic Coatings: A Systems Approach, ACS Symposium Series 722, Bauer, D.R. and Martin, J.W. (Eds.), American Chemical Society, Washington, DC, pp. 332–353, 1999.
Author information
Authors and Affiliations
Additional information
Building Materials Division, 100 Bureau Dr., Stop 8621, Gaithersburg, MD 20899-8621.
Rights and permissions
About this article
Cite this article
VanLandingham, M.R., Nguyen, T., Byrd, W.E. et al. On the use of the atomic force microscope to monitor physical degradation of polymeric coating surfaces. Journal of Coatings Technology 73, 43–50 (2001). https://doi.org/10.1007/BF02720133
Issue Date:
DOI: https://doi.org/10.1007/BF02720133