Abstract

The nitrogen solubility and aluminum nitride formation in liquid Fe-Al, Fe-Cr-Al, Fe-18 pct Cr-8 pct Ni-Al and Fe-18 pct Cr-8 pct Ni-Mo-Al alloys were measured by the Sieverts' method. The temperature range extended from 1823 to 2073 K, and the aluminum contents from 1.01 to 3.85 wt pct Al. Increasing aluminum content increases the nitrogen solubility. The effect of molybdenum additions was determined for 2, 4 and 8 wt pct Mo levels. The first and second order effects of chromium, nickel, molybdenum and aluminum on the activity coefficient of nitrogen in iron were determined. The first and second order effects of chromium, nickel and molybdenum on the activity coefficient of aluminum also were determined. The nitride precipitates were identified as stoichiometric aluminum nitride, AIN, by X-ray diffraction analysis. The lattice spacing was in good agreement with the ASTM standard patterns for AIN in both higher and lower Al content solutions. The solubility product of AIN increases with increasing aluminum concentration and with temperature in liquid iron and the iron alloys studied. However, the magnitudes of the solubility products of AIN in those alloys are different because of the effects of chromium and nickel additions. Additions of molybdenum show little effect on the solubility product of AIN. The standard free energy of formation of AIN in liquid iron is: δG‡ = -245,990 + 107.59 \T J/g-molAIN, based on the standard state of the infinitely dilute solution in liquid iron for aluminum and nitrogen, referred to a hypothetical one wt pct solution, and on the pure compound for A1N.

This is a preview of subscription content, log in via an institution to check access.

Access this article

Price excludes VAT (USA)
Tax calculation will be finalised during checkout.

Instant access to the full article PDF.

Similar content being viewed by others

References

  1. D. B. Evans and R. D. Pehlke:Trans. TMS-AIME, 1964, vol. 230, pp. 1651–56.

    CAS  Google Scholar 

  2. F. G. Jones, H. E. Gardner, and R. D. Pehlke:Ibid, 1968, vol. 242, pp. 2453- 56.

    CAS  Google Scholar 

  3. H. Wada and R. D. Pehlke:Met. Trans. B, 1977, vol. 8B, pp. 443–50.

    Article  CAS  Google Scholar 

  4. S. Maekawa, Y. Nakagawa, and Y. Yanagawa:Tetsu-to-Hagane, 1960, vol. 46, pp. 1438–41.

    CAS  Google Scholar 

  5. R. D. Pehlke and J. F. Elliott:Trans. TMS-AIME, 1960, vol. 218, pp. 1088- 1101.

    Google Scholar 

  6. C. H. Lupis and J. F. Elliott:Ibid, 1965, vol. 233, pp. 257–58.

    CAS  Google Scholar 

  7. H. Wada and R. D. Pehlke:Met. Trans. B, 1977, vol. 8B, pp. 675–82.

    CAS  Google Scholar 

  8. E. Ichise, T. Yamauchi, and T. Mori:Tetsu-to-Hagane, 1977, vol. 63, pp. 417- 24.

    Google Scholar 

  9. F. Woolley and J. F. Elliott:Trans. TMS-AIME, 1967, vol. 239, pp. 1872–83.

    CAS  Google Scholar 

  10. T. C. Wilder and J. F. Elliott:J. Electrochem. Soc, 1960, vol. 107, pp. 628- 35.

    Article  Google Scholar 

  11. J. Chipman and T. P. Florides:Acta Met., 1955, vol. 3, pp. 456–69.

    Article  CAS  Google Scholar 

  12. G. R. Belton and R. J. Fruehan:Trans. TMS-AIME, 1969, vol. 245, pp. 113–17.

    CAS  Google Scholar 

Download references

Author information

Authors and Affiliations

Authors

Rights and permissions

Reprints and permissions

About this article

Cite this article

Wada, H., Pehlke, R.D. Nitrogen solubility and aluminum nitride precipitation in liquid iron, Fe-Cr, Fe-Cr-Ni, and Fe-Cr-Ni-Mo alloys. Metall Trans B 9, 441–448 (1978). https://doi.org/10.1007/BF02654419

Download citation

  • Received:

  • Published:

  • Issue Date:

  • DOI: https://doi.org/10.1007/BF02654419

Keywords

Navigation