Abstract
Catalytic decomposition of N2O has been studied over a series of solid solution La2CuxZn1−xO4 (0<X≤1.0) at 200 Torr initial pressure of N2O, in the temperature range 330–490°C. The observed trends in the kinetics have been explained based on polaron hopping mechanism. Parallel variation between activity and magnetic susceptibility has been observed.
Abstract
Каталитическое разложение N2O исследовали на серии твердых растворов La2CuxZn1−xO4 (0<X≤1.0) при исходном давлении N2O 200 торр и при температурах 330–490°C. Наблюдаемые зависимости в кинетике объясняли на основе механизма перескакивания полярона. Наблюдали параллельное изменение в активности и магнитной восприимчивости.
Similar content being viewed by others
References
N. Gunasekaran, A. Meenakshisundaram, V. Srinivasan: Indian J. Chem.,21A, 346 (1982).
T. Arakawa: Mat. Res. Bull.,14, 507 (1979).
K. V. Ramanujachary, N. Kameswari, C. S. Swamy: J. Catal.,86, 121 (1984).
T. Nitadori, M. Misono: Chem. Lett., 1255 (1986).
K. V. Ramanujachary, C. S. Swamy: J. Catal.,93, 279 (1985).
U. Kameswari, C. S. Swamy: J. Mater. Sci. Lett.,4, 1515 (1985).
A. Cimino, V. Indovina, F. Pepe, F. S. Stone: Gazz. Chim. Ital.,103, 935 (1973).
P. Pomanis, J. C. Vickerman: J. Catal.,55, 88 (1978).
T. A. Ergerton, F. S. Stone, J. C. Vickerman: J. Catal.,33, 299 (1974).
Author information
Authors and Affiliations
Rights and permissions
About this article
Cite this article
Kameswari, U., Christopher, J. & Swamy, C.S. Studies on the catalytic decomposition of N2O over the solid solution La2CuxZn1−xO4 (0<X≤1.0). React Kinet Catal Lett 41, 381–388 (1990). https://doi.org/10.1007/BF02097898
Received:
Accepted:
Issue Date:
DOI: https://doi.org/10.1007/BF02097898