Advertisement

Journal of Materials Science Letters

, Volume 8, Issue 7, pp 771–776 | Cite as

Modelling the ageing phenomena in 0.9PMN-0.1PT relaxor ferroelectric ceramics

  • W. Y. Pan
  • T. R. Shrout
  • L. E. Cross
Article

Keywords

Polymer Ferroelectric Ceramic Ageing Phenomenon Relaxor Ferroelectric Ceramic 
These keywords were added by machine and not by the authors. This process is experimental and the keywords may be updated as the learning algorithm improves.

Preview

Unable to display preview. Download preview PDF.

Unable to display preview. Download preview PDF.

References

  1. 1.
    K. CARL and K. H. HARDTL,Ferroelectrics 17 (1978) 472.Google Scholar
  2. 2.
    W. A. SCHULZE, submitted toFerroelectrics. Google Scholar
  3. 3.
    K. W. PLESSNER,Proc. Phys. Soc. B 69 (1965) 1261.Google Scholar
  4. 4.
    H. DEDERICHS and G. ARLT,Ferroelectrics 68 (1986) 281.Google Scholar
  5. 5.
    W. A. SCHULZE, J. V. BIGGERS and L. E. CROSS,J. Amer. Ceram. Soc. 61 (1978) 46.Google Scholar
  6. 6.
    G. BORCHHARDT, J. Von GIEMINSKI and G. SCHMIDT,Phys. Status Solidi (a) 59 (1980) 747.Google Scholar
  7. 7.
    W. Y. PAN, E. FURMAN, G. O. DAYTON and L. E. CROSS,Mater. Lett. 5 (1986) 647.Google Scholar
  8. 8.
    N. SETTER and L. E. CROSS,J. Appl. Phys. 51 (1980) 4356.Google Scholar
  9. 9.
    G. A. SMOLENSKII and V. A. ISOPOV,Sov. Phys. Dokl. 9 (1964) 653.Google Scholar
  10. 10.
    S. L. SWARTZ and T. R. SHROUT,Mater. Res. Bull. 17 (1982) 1245.Google Scholar
  11. 11.
    M. YOKOSUKA and M. MARUTAKE,J. Appl. Phys. 25 (1986) 981.Google Scholar
  12. 12.
    M. C. McQUARRIE and W. R. BUESSEM,Amer. Ceram. Soc. Bull. 34 (1955) 402.Google Scholar
  13. 13.
    XI YAO, Z. CHEN and L. E. CROSS,J. Appl. Phys. 54 (1983) 3399.Google Scholar

Copyright information

© Chapman and Hall Ltd. 1989

Authors and Affiliations

  • W. Y. Pan
    • 1
  • T. R. Shrout
    • 1
  • L. E. Cross
    • 1
  1. 1.Materials Research LaboratoryThe Pennsylvania State UniversityUniversity ParkUSA

Personalised recommendations