Kempiraisk chromite makes it difficult for magnesiospinel articles to be sintered in the refractory-production furnaces. In order to obtain good quality periclase-chromite articles based on Kempiraisk chromite under the conditions pertaining at the Combine, it is necessary to coarsen the chromite fraction to 5–0.5 mm, reduce its concentration in the batch to 20–27%, and to increase the firing temperature to 1580–1590°C after first reconstructing the gas-fired chamber furnaces.

This is a preview of subscription content, log in via an institution to check access.

Access this article

Price excludes VAT (USA)
Tax calculation will be finalised during checkout.

Instant access to the full article PDF.

Similar content being viewed by others

Author information

Authors and Affiliations

Authors

Additional information

Translated from Ogneupory, No. 5, pp. 8–11, May, 1982.

Rights and permissions

Reprints and permissions

About this article

Cite this article

Kishenin, V.A., Pugachev, E.M., Strokova, L.I. et al. Use of Kempiraisk chromite for the production of magnesiospinel refractories. Refractories 23, 217–219 (1982). https://doi.org/10.1007/BF01387343

Download citation

  • Issue Date:

  • DOI: https://doi.org/10.1007/BF01387343

Keywords

Navigation