Conclusions
With the use of Arkalyksk clay in existing conditions of refractories production at the ChMZ plant for obtaining grog with a water absorption of up to 5–6% it is necessary to add 25% plastic clay of the Buskul'sk type.
The introduction into use of a rotary furnace will permit the firing of refractory Arkalyksk high-grade clays without additions, which should increase the life of the ladle and stopper refractories.
Similar content being viewed by others
Author information
Authors and Affiliations
Rights and permissions
About this article
Cite this article
Brodetskii, G.G., Karpova, N.D. Making refractory products from Arkalyksk clays. Refractories 5, 57–59 (1964). https://doi.org/10.1007/BF01290456