Conclusions
-
1.
Preliminary deformation of contacting samples does not change the rate and temperature of CM in nonsteady-diffusional conditions in the systems cadmium-lead-tin and cadmium-lead-bismuth.
-
2.
With change in grain size in the deformation of samples of the three-component systems cadmium-lead-tin and cadmium-lead-bismuth, the structure of the solid-phase-liquid boundary in CM in nonsteady diffusional conditions changes.
-
3.
The temperature and rate of CM in the three-component system cadmium-tin-lead changes from 145 to 168°C and from 6.2·10−2 to 1.52· 10−2 mm/min with increase in omnidirectional pressure from 1000 to 12,000 bar, while the microhardness of the contact layers rises by 24%.
Literature cited
P. A. Savintsev, I. K. Malkanduev, V. I. Rogov, and I. M. Temukuev, Fiz. Met. Metalloved.,37, No. 2, 438 (1974).
I. K. Malkanduev and S. P. Savintsev, Izv. Akad. Nauk SSSR, Met., No. 4, 72 (1975).
L. K. Savitskaya and P. A. Savintsev, in: Surface Phenomena in Melts and Powder-Metallurgy Processes [in Russian], Naukova Dumka, Kiev (1963), p. 273.
V. I. Rogov, Candidate's Dissertation, Nal'chik (1969).
N. N. Nilova, G. M. Bartenev, and V. T. Borisov, Dokl. Akad. Nauk SSSR,198, No. 5, 1060 (1971).
D. S. Kamenetskaya, I. A. Korsunskaya, and Yu. A. Litvin, Fiz. Met. Metalloved.,45, No. 2, 569 (1978).
Author information
Authors and Affiliations
Additional information
Translated from Izvestiya Vysshikh Uchebnykh Zavedenii, Fizika, No. 5, pp. 102–104, May, 1979.
Rights and permissions
About this article
Cite this article
Savintsev, P.A., Gavrilov, K.I. Effect of fusible-metal deformation on contact-melting kinetics. Soviet Physics Journal 22, 541–543 (1979). https://doi.org/10.1007/BF00893251
Received:
Revised:
Issue Date:
DOI: https://doi.org/10.1007/BF00893251