Conclusions
-
1.
It is shown that sheet material can be successfully rolled from powder containing up to 16 wt.% of graphite.
-
2.
To obtain strip with stable properties from a powder mixture with a solid lubricant filler, it is necessary to add glycerin to the charge. The optimum glycerin content depends on the amount of solid lubricant in the charge and the rolling process parameters.
Similar content being viewed by others
Literature cited
M. V. Mal'tsev and A. N. Nikolaev, Poroshk. Metall., No. 7 (1969).
G. A. Vinogradov, Yu. N. Semenov, O. A. Katrus, and V. P. Katashinskii, The Rolling of Metal Powders [in Russian], Metallurgiya, Moscow (1969).
R. Ya. Ponil'skii and F. V. Kondrashov, The Pressing of Ceramic Powders [in Russian], Metallurgiya, Moscow (1968).
Author information
Authors and Affiliations
Additional information
Translated from Poroshkovaya Metallurgiya, No. 10(166), pp. 9–13, October, 1976.
Rights and permissions
About this article
Cite this article
Paryshev, V.M., Shotkin, Y.A. Rolling of powder mixtures with a solid lubricant filler. Powder Metall Met Ceram 15, 746–749 (1976). https://doi.org/10.1007/BF00796187
Received:
Issue Date:
DOI: https://doi.org/10.1007/BF00796187