Literature cited
Yu. B. Paderno and V. V. Odintsov, “Preparation of metallic dodecarborides by borothermic reduction of metallic oxides,” in: Metallothermic Processes in Chemistry and Metallurgy [in Russian], Nauka, Novosibirsk (1971), pp. 39–43.
Author information
Authors and Affiliations
Additional information
Translated from Poroshkovaya Metallurgiya, No. 10(178), pp. 33–34, October, 1977.
Thus, in reduction reactions performed in a vacuum use should be made of blanks pressed under a certain optimum pressure, which for metallic dodecaborides is 90–120 kgf/cm2. This shortens synthesis time and enables single-phase materials to be obtained.
Rights and permissions
About this article
Cite this article
Odintsov, V.V., Moiseenko, L.L. Dependence of the degree of completeness and duration of the borothermic reduction reaction on compact density in the preparation of metallic dodecaborides. Powder Metall Met Ceram 16, 766–767 (1977). https://doi.org/10.1007/BF00793583
Received:
Issue Date: