A point pressure gauge giving a sensitivity of 4 or 16 N/cm2 has been designed and constructed.

It has been established that, in the rolling of metal powders, powder densification under the influence of the forces exerted by the rolls takes place over an arc of not more than 20°.

This is a preview of subscription content, log in via an institution to check access.

Access this article

Price excludes VAT (USA)
Tax calculation will be finalised during checkout.

Instant access to the full article PDF.

Similar content being viewed by others

Literature cited

  1. A. P. Chekmarev, P. L. Klimenko, and G. A. Vinogradov, Tr. LPI, No. 222, Mashgiz (1963).

  2. G. A. Vinogradov and V. P. Katashinskii, Poroshkovaya Met., No. 9 (1965).

  3. V. G. Khromov, Tr. LPI, No. 222, Mashgiz (1963).

  4. V. P. Katashinskii and G. A. Vinogradov, Poroshkovaya Met., No. 5 (1965).

Download references

Author information

Authors and Affiliations

Authors

Additional information

Translated from Poroshkovaya Metallurgiya, No. 7 (67), pp. 19–21, July, 1968.

Rights and permissions

Reprints and permissions

About this article

Cite this article

Katashinskii, V.P. Length of the densification zone in metal powder rolling. Powder Metall Met Ceram 7, 523–524 (1968). https://doi.org/10.1007/BF00774697

Download citation

  • Received:

  • Issue Date:

  • DOI: https://doi.org/10.1007/BF00774697

Keywords

Navigation