Properties of sinter with a basicity of 0.6–3.4

  • Pig iron
  • Published:
Metallurgist Aims and scope

This is a preview of subscription content, log in via an institution to check access.

Access this article

Price excludes VAT (USA)
Tax calculation will be finalised during checkout.

Instant access to the full article PDF.

Authors

Additional information

Chelyabinsk Scientific-Research Institute of Metallurgy, Chelyabinsk Metallurgical Works. Translated from Metallurg, No. 9, pp. 3–5, September, 1970.

Rights and permissions

Reprints and permissions

About this article

Cite this article

Fedorenko, N.V., Sokolevskikh, G.F., Rusakova, A.G. et al. Properties of sinter with a basicity of 0.6–3.4. Metallurgist 14, 552–554 (1970). https://doi.org/10.1007/BF00733727