Conclusions
Plates of alloy VAD23 should be produced by treatment III with hot rolling at 400–490°, ensuring the necessary quality of the plates and the mechanical properties.
Similar content being viewed by others
Literature cited
K. N. Mikhailov et al., "Production technique and mechanical properties of plates of alloy VAD23", in: Aluminum Alloys. No. 4. Heat-Resistant and High-Strength Alloys [in Russian], Metallurgiya, Moscow (1966), p. 65.
Commercial Wrought, Sintered, and Cast Aluminum Alloys. Handbook [in Russian], Metallurgiya, Moscow (1972), p. 211.
Additional information
Translated from Metallovedenie i Termicheskaya Obrabotka Metallov, No. 12, pp. 58–61, December, 1978.
Rights and permissions
About this article
Cite this article
Kolobnev, N.I., Ovodenko, M.B., Shivrin, G.T. et al. Effect of thermomechanical parameters on the structure and properties of plates of alloy VAD23. Met Sci Heat Treat 20, 1031–1034 (1978). https://doi.org/10.1007/BF00703287