When the annealing time at 650°C is extended to 6–7 h, the base texture (0001) [10 10] forms in sheets of titanium alloys PT-3V and PT-3Vkt, and this enhances the pressability of the sheets and the strength of the products made from them.
Similar content being viewed by others
Literature cited
R. A. Adamesku, A. A. Alsagarov, P. V. Gel'd, et al., "Texture and pressability of sheets of alloy VT6," Tekhnol. Legkikh Splavov, No. 11, 67–68 (1976).
A. W. Bowen, "On the importance of crystallographic texture in the characterization of alpha-based titanium alloys," Scr. Met.,11, 17–21 (1977).
H. W. Babel and S. F. Frederick, "A review of texture strengthening of titanium alloys," J. Met.,20, 32–38 (1968).
D. A. Skryabin, S. R. Rusetskii, and R. A. Adamesku, "The effect of alloying on the temperature of onset of recrystallization of titanium alloys," Tekhnol. Legkikh Splavov, No. 1, 43–45 (1975).
R. A. Adamesku, D. A. Skryabin, Yu. S. Bratchikov, et al., Formation of the recrystallization texture in titanium-aluminum alloys, in: Titanium, Metal Science and Technology: Transactions of the 3rd International Conference on Titanium (Moscow, 1976), Vol. 3, Moscow (1978), pp. 103–110.
G. Gleiter and B. Chalmers, Large-Angle Grain Boundaries [Russian translation], Mir, Moscow (1975).
Additional information
Ural Polytechnic Institute. Ural Electromechanical Institute of Railroad Transport Engineers. Translated from Metallovedenie i Termicheskaya Obrabotka Metallov, No. 7, pp. 53–54, July, 1990.
Rights and permissions
About this article
Cite this article
Adamesku, R.A., Grebenkin, S.V., Polikarpov, E.Y. et al. Effect of the length of annealing on the texture of sheets of titanium alloys PT-3V and PT-3Vkt. Met Sci Heat Treat 32, 535–537 (1990). https://doi.org/10.1007/BF00700328
Issue Date:
DOI: https://doi.org/10.1007/BF00700328