Effect of an inhibiting layer on critical crack length and fracture toughness of D16T alloy sheet during cyclic loading

  • V. M. Grigor'ev
  • V. P. Turko
Strength Properties


Treatment of D16T alloy sheet in cold phosphating inhibiting solution does not lead to an increase in critical crack length and does not worsen material fracture toughness.


Fracture Toughness Crack Length Cyclic Loading Alloy Sheet Critical Crack 
These keywords were added by machine and not by the authors. This process is experimental and the keywords may be updated as the learning algorithm improves.


Unable to display preview. Download preview PDF.

Unable to display preview. Download preview PDF.

Literature cited

  1. 1.
    V. S. Ivanova and V. G. Kudryashov, in: Fatigue and Brittleness of Metallic Materials [in Russian], Metallurgiya, Moscow (1968).Google Scholar
  2. 2.
    V. G. Kudryashov and V. I. Smolentsev, Fracture Toughness of Aluminum Alloys [in Russian], Metallurgiya, Moscow (1976).Google Scholar
  3. 3.
    G. A. Korn and T. M. Korn, Manual of Mathematics, McGraw-Hill (1967).Google Scholar

Copyright information

© Plenum Publishing Corporation 1981

Authors and Affiliations

  • V. M. Grigor'ev
  • V. P. Turko

There are no affiliations available

Personalised recommendations