Conclusions
Restoring worn parts with Sv. 08A welding wire and AN348A flux with 5% silicon carbide added to it increases the wear resistance and reduces the cost of the facing as compared with P-1 and NP30KhGSA welding wires.
Similar content being viewed by others
Literature cited
N. F. Grokhol'skii, Restoring Machine Parts by Hard-Facin [in Russian], Mashgiz, Moscow (1962).
Additional information
Volgorad Agricultural Institute. Translated from Metallovedenie in Termicheskaya Obrabotka Metallov, No. 7, pp. 39–40, July, 1968.
Rights and permissions
About this article
Cite this article
Suchkov, O.K., Kondrat'ev, E.T. & Emel'yanov, V.A. Restoring worn machine parts by hard facing. Met Sci Heat Treat 10, 535 (1968). https://doi.org/10.1007/BF00654361