Abstract
Influences of sintering conditions onT c are studied for Bi1.6Pb0.4Sr2Ca2(Cu0.9Ti0.1)3Ox. HighT c values are obtained at 1123±5 K sintering temperature and over 50 h sintering time. In order to explain theT c changes, morphological discussion is attempted.
Similar content being viewed by others
References
Y. Nishi, S. Moriya andT. Manabe,J. Appl. Phys. 65 (1989) 2389.
Y. Nishi, K. Oguri, H. Ohinata, K. Tanioka, Y. Kita andN. Ninomiya,Phys. Rev. B 41 (1990) 6520.
Y. Nishi, Y. Kita andK. Tanioka,J. Mater. Sci. 25 (1990) 5105.
Y. Nishi, K. Nozaki, T. Kurotaki, Y. Kita andK. Oguri,J. Appl. Phys. 71 (1992) 350.
M. Onoda, A. Yamamoto, E. Takayama-Muromachi andS. Takekawa,Jpn J. Appl. Phys. 27 (1988) L833.
U. Endo, S. Koyama andT. Kawai,ibid. 27 (1988) L1476.
Author information
Authors and Affiliations
Rights and permissions
About this article
Cite this article
Nishi, Y., Nozaki, K., Kurotaki, T. et al. Formation of high-T c Bi1.6Pb0.4Sr2Ca2(Cu0.9Ti0.1)3Ox . J Mater Sci 28, 5262–5264 (1993). https://doi.org/10.1007/BF00570075
Received:
Accepted:
Published:
Issue Date:
DOI: https://doi.org/10.1007/BF00570075