The effect of the form of chromium-plated fibre-conducting equipment in the KV-III-250 KA machine on the properties of polycaproamide yarn of 187 tex linear density which has been treated with lubricant Teprém-6 is described.

It is recommended to use “worn-in” stretch rolls with a matte surface for their lower stretch rolls; for the heat-plasticizers and other parts, where it is advisable to have a low coefficient of yarn friction, it is recommended to use a shiny-rough surface.

This is a preview of subscription content, log in via an institution to check access.

Access this article

Price excludes VAT (USA)
Tax calculation will be finalised during checkout.

Instant access to the full article PDF.

Similar content being viewed by others

Literature cited

  1. G. I. Yakimenko, A. I. Solyar, and I. S. Bondarchuk, Zavod. Lab., No. 8, 991 (1975).

Download references

Authors

Additional information

Translated from Khimicheskie Volokna, No. 2, pp. 57–59, March–April 1984.

Rights and permissions

Reprints and permissions

About this article

Cite this article

Perevalova, N.A., Gusakov, M.Y., Rumyantsev, R.A. et al. Service properties of chrome-plated surface of fibre-guiding equipment in the KV-III-250 KA machine. Fibre Chem 16, 125–127 (1984). https://doi.org/10.1007/BF00555889

Download citation

  • Received:

  • Issue Date:

  • DOI: https://doi.org/10.1007/BF00555889

Keywords

Navigation