Acid treatment of polyacrylonitrile tows with subsequent high-temperature washing

  • É. R. Alieva
  • Yu. P. Kozhevnikov
  • V. A. Medvedev
  • A. T. Serkov
Chemistry And Technology Of Man-Made Fibres
  • 38 Downloads

Conclusions

-- A method has been proposed for combined short-term acid treatment of polyacrylonitrile tow with a sulfuric acid solution of elevated concentration. Intensification of the process of acid diffusion is achieved by subsequent high-temperature washing.

-- The process of combined acid treatment and washing of fibre has been studied in which washing begins before completion of acid diffusion to the tow axis. It has been shown that in acid treatment during the course of the reduced time of 0.4 · 104 sec/cm2 (which corresponds to 0.5–2 sec) and subsequent washing with water having a temperature of 50–60°C, complete acid treatment of the tow is achieved.

Keywords

Polymer Sulfuric Acid Acid Solution Acid Treatment Elevated Concentration 
These keywords were added by machine and not by the authors. This process is experimental and the keywords may be updated as the learning algorithm improves.

Preview

Unable to display preview. Download preview PDF.

Unable to display preview. Download preview PDF.

Literature cited

  1. 1.
    News in the Region of Viscose Fibre Manufacturing [in Russian], Sb. Nauch. tr. pod red. A. T. Serkova, Mytishchi (1986), p. 4.Google Scholar

Copyright information

© Plenum Publishing Corporation 1992

Authors and Affiliations

  • É. R. Alieva
  • Yu. P. Kozhevnikov
  • V. A. Medvedev
  • A. T. Serkov

There are no affiliations available

Personalised recommendations