Conclusions
Procedures have been developed for the potentiometric determination of BSA content of impregnating baths and on the surface of fillers in the technological process of making chemically resistant tubes.
The procedures proposed are characterized by accuracy and reproducibility of results.
A study of the change in BSA content and moisture content at various stages of the technological process of making chemically resistant tubes has shown a change in the figures for these indices with the storage time of the starting BSA and of the impregnating solutions, and with filler nonuniformity.
Similar content being viewed by others
Literature cited
E. A. Gribova, Zav. Lab., No. 11, 1356–1358 (1958).
G. I. Svistunova, Zav. Lab., No. 6, 548–549 (1962).
A. D. Igoshev and V. N. Lukashenok, Zav. Lab., No. 2, 155–156 (1973).
L. N. Bykova, M. G. Khusainov, et al., Khim. Volokna, No. 4, 73–75 (1978).
Additional information
Translated from Khimicheskie Volokna, No. 1, pp. 56–57, January–February, 1987.
Rights and permissions
About this article
Cite this article
Matveiko, L.V., Bogoslovskaya, T.N., Chernousova, N.I. et al. Potentiometric determination of benzenesulfonic acid in technological solutions and on the surface of fillers. Fibre Chem 19, 78–81 (1987). https://doi.org/10.1007/BF00544630
Received:
Issue Date:
DOI: https://doi.org/10.1007/BF00544630