Summary
The dielectric relaxation processes in poly(azourethaneurea) prepared from diphenylmethane-4,4′-diisocyanate (MDI) and poly(ethylene adipate) glycol were studied in the range 200–390 K using thermally stimulated depolarization currents (TSDC). The TSDC spectra obtained on original sample, annealed sample, and both annealed and stretched sample showed significant differences which were explained in terms of the supramolecular structure of polymers. It was accepted that the polymers have a multiphase supramolecular structure.
Similar content being viewed by others
References
I. Diaconu, C. Ciobanu and Cr.I. Simionescu, Polym. Bull., 20, 195(1988)
I. Diaconu, C. Ciobanu and Cr.I. Simionescu, Polym. Bull., 21, 203(1989)
I.Diaconu, C.Ciobanu and Cr.I.Simionescu,Europ.Polym.J., accepted for publication, 1989
C.E. Wilkes and C.S. Yusek, J. Macromol. Sci.-Phys., B7(1), 157(1973)
C.Ciobanu and I.Diaconu, to be published, 1990
I. Diaconu and S. Dumitrescu, Europ. Polym. J., 14, 971(1979)
Author information
Authors and Affiliations
Rights and permissions
About this article
Cite this article
Diaconu, I., Ciobanu, C. & Simionescu, C.I. Properties of urethane elastomers. Polymer Bulletin 24, 573–576 (1990). https://doi.org/10.1007/BF00395582
Accepted:
Issue Date:
DOI: https://doi.org/10.1007/BF00395582