Summary
The thermally stimulated depolarization currents from poly(2-ethynylnaphtalene) with cis-cisoidal and transcisoidal structures were studied over the temperature range 200–380 K. The single peak ρ of the cis-cisoidal isomer was assigned to the Maxwell-Wagner polarization. The β1 and β2 peaks of the trans-cisoidal isomer arise from a single dipolar relaxation process and respectively from a dipolar relaxation distributed in natural frequency. Certains assignements are based on comparative work on polyphenylacetylene.
Similar content being viewed by others
References
BUCCI C., FIESHI R. and GUIDI G., Phys.Rev.,148,816(1966)
CHIANG C.K.,FINCHER C.R.Jr.,PARK Y.W.,HEEGER A.J., SHIRAKAWA H.,LOUIS E.J.,GAU S.C. and MacDIARMID A.G., Phys.Rev.Lett., 39, 1098 (1977)
CHIANG C.K.,DRUY M.A., GAU S.C., HEEGER A.J., SHIRAKAWA A.H.,LOUIS E.J.,MacDIARMID A.G. and PARK Y.W., J.Am. Chem.Soc., 100, 1013 (1978)
CUKOR P., KRUGLER I. and RUBNER M., Macromol.Chem.Phys., 182, 165 (1981)
DEITS W., CUKOR P., RUBNER M. and JOPSON H., Polym.Prep., 22, 197 (1981)
DIACONU I. and DUMITRESCU Sv., Eur.Polym.J., 14, 971 (1978)
DIACONU I. and DUMITRESCU Sv., Eur.Polym.J., 15, 1155 (1979)
DIACONU I. and DUMITRESCU Sv., Eur.Polym.J., 16, 511 (1980)a
DIACONU I. and DUMITRESCU Sv., Bul.Inst.Politeh.Iaşi, Secţia II, XXVI, 63 (1980)b
DIACONU I., DUMITRESCU Sv. and SIMIONESCU Cr., Eur.Polym. J., 16, 515 (1980)
DIACONU I., DUMITRESCU Sv. and SIMIONESCU Cr., Polym. Bul., 4, 535 (1981)
DIACONU I. and DUMITRESCU Sv., J.Macromol.Sci.-Phys., 21, 555 (1982)
SIMIONESCU Cr., DUMITRESCU Sv., PERCEC V., Polym.J., 8, 139 (1976)
Author information
Authors and Affiliations
Rights and permissions
About this article
Cite this article
Diaconu, I., Dumitrescu, S. Dielectric relaxation in poly(2-ethynylnaphtalene) determined by thermally stimulated depolarization currents. Polymer Bulletin 9, 17–20 (1983). https://doi.org/10.1007/BF00275562
Received:
Revised:
Accepted:
Issue Date:
DOI: https://doi.org/10.1007/BF00275562