Summary
A water soluble polyacrylic acid has been obtained by polymerization of acrylic acid initiated with silica-supported poly-γ-mercaptopropylsiloxane in the presence of water and carbon tetrachloride. A super absorbent sodium polyacrylate (water absorbing capacity 300 g/g) has been prepared by copolymerization of acrylic acid with a small amount of p-divinylbenzene with the same initiator in a mixture of aqueous sodium hydroxide solution, carbon tetrachloride, n-hexane and Tween 80.
Similar content being viewed by others
References
ARAKI, N.: Synthetic Polymers III, Asakura, Tokyo,219(1971)
GUGLIEMELLI, L.A., GUGLIEMELLI, M.O., RUSSELL, C.R., RIST, C.E.: J. Appl. Polym. Sci., 13,2007 (1969)
DOW CHEM.: U.S. Pat., 3,247,171(1966)
UNION CARBIDE: Japan 27,039(1973)
KAO SOAP: Japan Kokai, 46,389(1978)
INDUSTRIAL RESEARCH INSTITUTE: Japan Kokai, 55,647(1975)
DOW CHEM.: U.S. Pat., 3,669,103(1972)
Author information
Authors and Affiliations
Rights and permissions
About this article
Cite this article
Huang, M.Y., Wu, R. & Jiang, L.R. Polymerization of acrylic acid initiated with poly-γ-mercaptopropylsiloxane. Polymer Bulletin 9, 5–10 (1983). https://doi.org/10.1007/BF00275560
Received:
Accepted:
Issue Date:
DOI: https://doi.org/10.1007/BF00275560