Summary
The study was carried out in order to determine the effects of CCA on the pyrolysis and the combustion toxicity of wood. The results from CCA treated wood are summarized as follows: 1. CCA accelerated the beginning of pyrolysis of wood, increased the activation energies for the weight loss by pyrolysis, and increased the char yields in both air and helium. 2. Almost all the original amounts of cromium and copper were retained in the ash while some of the arsenic evolved into the gas phase, which increased with increasing temperature and air supply. 3. The combustion toxicity of wood samples was affected more by the sample density and CO concentration than CCA. It is concluded that for minimizing gaseous toxicants from arsenic, CCA treated wood must be burned at low temperatures with a reduced air supply.
Similar content being viewed by others
References
Akita, K; Kase, M. 1976: Determination of kinetic parameters for pyrolysis of cellulose and cellulose treated with ammonium phosphate by differential thermal analysis and thermal gravimetric analysis. J. Polymer Sci., A-1 5:833–848
Appel, B. R.; Tokiwa, Y; Hoffer, E. M. 1984: Efficiency of filter sampling for arsenic in the atmosphere. Atmos. Env. 18:219–222
Dahlgren, S.-E. 1974: Kinetics and mechanism of fixation of Cu-Cr-As wood preservatives IV. Conversion reactions during storage. Holzforsch. 28:58–61
Hartzell, G. E.; Priest, D. N.; Switzer, W. G. 1985: Modeling of toxicological effects of fire gases: II. Mathematical modeling of intoxication of rats by carbon monoxide and hydrogen cyanide. J. Fire Sci. 3:115–128
Hirata, T. 1979: Changes in degree of polymerization and weight of cellulose untreated and treated with inorganic salts during pyrolysis. Bull. Forestry Forest Products Res. Inst. 203:77–124
Hirata, T.; Fukui, Y.; Kawamoto, S. 1988a: Plywood fire-retarded by chemical treatments I. Surface flammability. J. Japan Wood Res. Soc. 34:337–345
Hirata, T.; Kawamoto, S. 1988 b: Toxic gases from combustion of wood treated with retardants. 9th Joint Panel Meeting of UJNR Panel on Fire Research and Safety, NBSIR 88-3753, National Bureau of Standards, pp. 417–427
Hirata, T.; Kawamoto, S; Okuro, A. 1991a: Pyrolysis of melamine-formaldehyde and urea-formaldehyde resins. J. Appl. Polymer Sci. 42:3147–3163
Hirata, T.; Fukui, Y.; Kawamoto, S.; Karasawa, H. 1991b: Combustion gas toxicity, hygroscopicity, and adhesive strength of plywood treated with flame retardants. Wood Sci. Technol. 26:461–473
Hirata, T.; Kawamoto, S; Nishimoto, T. 1991c: Thermogravimetry of wood treated with water-insoluble retardants and a proposal for development of fire-retardant wood materials. Fire Materials 15:27–36
Sakurai, T. 1986: Studies on toxicity of single and multiple gases atmospheres. Proc. Ann. Meeting Japanese Assoc. Fire Sci. Engineering, Tokyo, pp. 107–110
Uesugi, S.; Fukui, Y; Abe, H. 1981: Combustive gas toxicity test for wood treated with chemicals. J. Japan Wood Res. Soc. 27:428–436
World Health Organization 1981: Arsenic — Environmental Health Criteria 18, World Health Organization, Geneva, p. 18 and 140
Author information
Authors and Affiliations
Rights and permissions
About this article
Cite this article
Hirata, T., Inoue, M. & Fukui, Y. Pyrolysis and combustion toxicity of wood treated with CCA. Wood Sci.Technol. 27, 35–47 (1992). https://doi.org/10.1007/BF00203408
Received:
Issue Date:
DOI: https://doi.org/10.1007/BF00203408