The effect of stylolites on the deterioration of limestone: possible mechanisms of damage evolution

  • Nevin Aly
  • Timothy Wangler
  • Ákos Török
Thematic Issue
  • 117 Downloads
Part of the following topical collections:
  1. Stone in the Architectural Heritage: from quarry to monuments – environment, exploitation, properties and durability

Abstract

This study presents five different lithotypes of limestone containing stylolites and commonly used as dimension stones in Egypt, Hungary and Israel. All the studied limestones are generally hard, dense, with high degree of cementation and have high strength and low porosity. Stylolites are small tooth-like irregular surfaces most often developed on the carbonate-rich stones. Insoluble particles, i.e., organic matter, oxides and clays are usually incorporated within the stylolitic planes. The presence of stylolites and their filling materials generally has a large effect on the physical and mechanical properties of the host stones. The main aim of this study is to evaluate the damage mechanism of different stylolitic limestones and to understand the role of the clay in the deterioration of these stones. Hundred cube samples (2 cm) of all the studied limestones were subjected to 500 thermal cycles (10–70 °C) and 20 cube samples (3 cm) of a grey Israeli limestone with high open porosity were subjected to multiple wet/dry cycles. The changes in mass, strength, and ultrasound Vp velocity, were measured to follow any damage that happened due to cycling. The thermal cycling was proved to be an effective deterioration mechanism of both Egyptian and Hungarian lithotypes. The response of Israel grey lithotype to the wet/dry cycling was clearly shown by the splitting of the tested samples through the stylolite planes and the sharp decrease of their strength.

Keywords

Stone decay Stylolites Clays Limestone Thermal cycles Wet/dry cycles 

Notes

Acknowledgements

Nevin Aly was supported by the Swiss Government excellence postdoctoral scholarship (2016.0766/Aegypten/OP. The authors would like to thank Dr. Thibault Demoulin from the Institute for Building Materials, D-BAUG – ETH Zurich, for helping during the DMA measurements. Thanks are also given to Dr. Ayman Hamad from the Faculty of Petroleum and Mining Engineering, Suez University, Egypt, for his helpful suggestions during the work. The financial support of Hungarian National Research, Development and Innovation (NKFI) Fund (no. K 116532) to AT is appreciated. The authors also thank an anonymous reviewer for his valuable suggestions that improved the manuscript.

References

  1. Bates RL, Jackson JA (1987) Glossary of geology. 3rd ed., American Geological InstituteGoogle Scholar
  2. Berthonneau J, Bromblet P, Cherblanc F, Ferraged, EVallet, J-M, Graubya O (2017) The spalling decay of building bioclastic limestones of Provence (South East of France): From clay minerals swelling to hydric dilation. J Cult Heritage 17:53–60CrossRefGoogle Scholar
  3. Camuffo D, Vincenzi S, Pilan L (1984) A first-order analysis of the heat wave in the soil. Water Air Soil Pollut 23:441–454CrossRefGoogle Scholar
  4. Davis GH, Reynolds SJ (1996) Structural geology of rocks and regions, 2nd edn. Wiley, New YorkGoogle Scholar
  5. De Boever W, Diaz A, Derluyn H, De Kock T, Van Stappen J, Dewanckele J, Bultreys T, Boone M, De Schryver T, Skjønsfjell ETB, Holler M, Breiby DW, Cnudde V (2015) Characterization of composition and structure of clay minerals in sandstone with ptychographic X-ray nanotomography. Appl Clay Sci 118:258–264CrossRefGoogle Scholar
  6. De Kock T, Turmel A, Fronteau G, Cnudde V (2017) Rock fabric heterogeneity and its influence on the petrophysical properties of a building limestone: Lede stone (Belgium) as an example. Eng Geol 216:31–41CrossRefGoogle Scholar
  7. Demoulin T, Girardet F, Wangler T, Scherer G, Flatt RJ (2016) On-site monnitoring for better selection of stone repairs: a case study. Her Sci 4:38CrossRefGoogle Scholar
  8. Friedman GM, Sanders JE (1972) Origin and occurrence of dolostones. Prentice Hall Incorporated, New YorkGoogle Scholar
  9. Gomez-Heras M, Smith BJ, Fort R (2006) Surface temperature differences between minerals in crystalline rocks: implications for granular disaggregation of granites through thermal fatigue. Geomorphology 78:236–249CrossRefGoogle Scholar
  10. Gutiérrez J, Mas A, Gil E, Galvañ V (2012) Clay-related damage in rainscreen walls built with natural stone coverings. Constr Build Mater 29:357–367CrossRefGoogle Scholar
  11. Hajpál M, Török Á (2004) Physical and mineralogical changes in sandstones due to fire and heat. Environ Geol 46(3):306–312Google Scholar
  12. Harvey RD (1966) Thermal expansion of certain Illinois limestones. Illinois State Geological Survey. Industrial Minerals Notes No 24:1–40Google Scholar
  13. Hockman A, Kessler DW (1950) Thermal and moisture expansion studies of some domestic granite. National Bureau of Standards, RP 2087Google Scholar
  14. Jimenez Gonzalez I, Scherer G (2004) Effect of swelling inhibitors on the swelling and stress relaxation of clay bearing stones. Env Geo 46(3–4):364–377Google Scholar
  15. Jiménez-González I, Rodriguez-Navarro C, Scherer GW (2008) Role of clay minerals in the physicomechanical deterioration of sandstone. J Geophys Res 113:F0202CrossRefGoogle Scholar
  16. Karatasios I, Theoulakis P, Kalagri A, Sapalidis A, Kilikoglou V (2009) Evaluation of consolidation treatments of marly limestones used in archaeological monuments. Construct Build Mater 23(8):2803–2812.  https://doi.org/10.1016/j.conbuildmat.2009.03.001 CrossRefGoogle Scholar
  17. Koch A, Siegesmund S (2006) The combined effect of moisture and temperature on the anomalous expansion behavior of marble. Env Geo 46(3–4):350–363Google Scholar
  18. Lapedes DN (ed) (1978) McGraw-Hill Encyclopedia of Geological Sciences. McGraw-Hill, p 915Google Scholar
  19. Larbi JA (2003) Effect of stylolites on durability of building stones: two case studies. HERON 48(3):231–247Google Scholar
  20. Molina E, Benavente D, Sebastian E, Cultrone G (2015) The influence of rock fabric in the durability of two sandstones used in the Andalusian Architectural Heritage (Montoro and Ronda, Spain). Eng Geol 197:67–81CrossRefGoogle Scholar
  21. Poppe LJ, Paskevich VF, Hathaway JC, Blackwood DS (2001) A laboratory manual for X-ray powder differaction. U.S. Geological Survey open-File Report 01–041Google Scholar
  22. Rodriguez-Navarro C, Sebastian E, Doehne E, Ginell WS (1998) The role of sepiolite-palygorskite in the decay of ancient Egyptian limestone sculptures. Clays Clay Miner 46(4):414–422CrossRefGoogle Scholar
  23. Roushdy M, Hammed MS, Abdel-Motelib A (2017) Geothenical porperties of Galala Limestone Tiles, Eocene rocks, Ain El Sukhna, Red Sea Coast, Egypt. Int J Chem Tech Res 10(5):368–378Google Scholar
  24. Ruedrich J, Bartelsen T, Dohrmann R, Siegesmund S (2011) Moisture expansion as deteioration factor for sandstone used in buildings. Env Ear Sci 63(7–8):1545–1564CrossRefGoogle Scholar
  25. Sebastian E, Benavente CultroneG, Fernandez D, Elert LL, Rodriguez-Navarro K (2008) Swelling damage in clay-rich sandstones usedin the church of San Mateo in Tarifa (Spain). J Cult Heritage 9:66–76CrossRefGoogle Scholar
  26. Smith BJ, Srinivasan S, Gomez-Heras M, Basheer PAM, Viles H (2011) Near-surface temperature cycling of stone and its implications for scales of surface deterioration. Geomorpohology 130:76–82CrossRefGoogle Scholar
  27. Tiennot M, Mertz JD, Bourges A (2017) Influence of anisotropic microcracking due to swelling on the fracture toughness of a clay-bearing sandstone. Rock Mech Eng 50(11):2861–2870CrossRefGoogle Scholar
  28. Török Á (2006) Influence of fabric on the physical properties of limestones. In: Kourkoulis SK (ed) Fracture and failure of natural building stones. Springer, Dordrecht, pp 487–495CrossRefGoogle Scholar
  29. Török Á (2007) Hungarian dimensional stones: an overview. Zeitschrift der Deutschen Gesellschaft für Geowissenschaften 158(3):361–374CrossRefGoogle Scholar
  30. Wangler T, Stratulat A, Duffus P, Prevost JH, Scherer G (2011) Flaw propagation and buckling in clay-bearing sandstones. Env Ear Sci 63(7–8):1565–1572CrossRefGoogle Scholar
  31. Wangler T, Sanchez A, Peri A (2016) Rapid degradation of stylolitic limestones used in Building cladding panels. 13th International Congress on the Deterioration and Conservation of Stone proceedings. The University of the West of Scotland, Glasgow 6–10 Sept. 2016Google Scholar
  32. Warke PA, Smith BJ (1994) Short-term rock temperature fluctuations under simulated hot desert conditions: some preliminary data. In: Robinson DA, Williams RBG (eds) Rock weathering and landform evolution. Wiley, Chichester, pp 57–70Google Scholar

Copyright information

© Springer-Verlag GmbH Germany, part of Springer Nature 2018

Authors and Affiliations

  1. 1.ETH ZurichInstitute for Building MaterialsZurichSwitzerland
  2. 2.Faculty of Petroleum and Mining EngineeringSuez UniversitySuezEgypt
  3. 3.Department of Engineering Geology and GeotechnicsBudapest University of Technology and EconomicsBudapestHungary

Personalised recommendations