Catalytic activity of CrO3/SiO2 samples for 2-propanol conversion is governed by only a small amount of active centers (estimated to be around 1017 per gram of catalyst), whereas excess chromium neither develops catalytic activity nor inhibits the reaction on the active sites. Only when the chromium loading is high enough to allow formation of bulk-like agglomerates (5 wt.% Cr) is 2-propanol converted also on this CrOx surface phase, but with a significant higher activation energy.
Keywords
Physical Chemistry Chromium Activation Energy Catalysis Catalytic ActivityAbstract
Каталитическая активность образцов CrO3/SiO2 для превращения 2-пропанола обуславливается лишь небольшим количеством активных центров (оцениваемое около 1017 на грамм катализатора), в то время как избыток хрома и не повышает каталитическую активность и не ингибирует реакциь на активных центрах. Лишь тогда, когда загрузка хрома достаточно высока чтобы позволить образование блоко-подобных агломератов (5 вес.% Cr), 2-пропанол превращается также на этой CrOx поверхностной фазе, но со значительно более высокой энергией активации.
Preview
Unable to display preview. Download preview PDF.
References
- 1.B. Parlitz, W. Hanke, R. Fricke, M. Richter, U. Roost, G. Öhlmann: J. Catal. (in press).Google Scholar
- 2.M. Richter, D. Mihajlova, G. Mrkwitschka, G. Öhlmann: (in preparation).Google Scholar
- 3.B. I. Baglai, K.M. Vaisberg, M.F. Mazitov, P.M. Masagutov: Proc. 5th Soviet Conf. on Modeling of Chem. and Oilconverting Processes and Reactors, Ufa 1974, p. 13.Google Scholar
- 4.J.P. Hogan: in “Applied Industrial Catalysis”, Vol. 1, p. 149 B.E. Leach ed., New York 1983.Google Scholar