Peel strengths at room temperature and under superplastic forming conditions at 530 °C were measured for diffusion-bonded joints in Al-Li 8090 alloy sheet. The bonds were made in the solid state, or via a transient liquid phase using interlayers. The effect of strain rate, sheet thickness and heat treatment were investigated. The significance of these results for the testing of DB joints and for their use in DB/SPF structures is discussed.
Keywords
Polymer Heat Treatment Liquid Phase Solid State Fracture Behaviour
These keywords were added by machine and not by the authors. This process is experimental and the keywords may be updated as the learning algorithm improves.
Preview
Unable to display preview. Download preview PDF.
References
- 1.R. Grimes, B. J. Dunwoody andJ. A. Jones, in “Superplasticity in Metals, Ceramics and Intermetallics”, Vol. 196, edited by M. J. Mayo, M. Kobayashi and J. Wadsworth (Materials Research Society, PA, 1990) pp. 167–72.Google Scholar
- 2.
- 3.D. W. Livesey andN. Ridley, “Diffusion Bonding 2”, edited by D. J. Stephenson (Eisevier, 1991) pp. 83–100.Google Scholar
- 4.R. A. Ricks, G. J. Mahon, N. C. Parsons, T. Heinrich andP.-J. Winkler,ibid., pp. 69–82.Google Scholar
- 5.
- 6.D. Stephen, “Designing with Titanium” (Institute of Metals, London, 1986) pp. 108–24.Google Scholar
- 7.
- 8.
- 9.
- 10.A. J. Kinloch, “Adhesion and Adhesives: Science and Technology” (Chapman and Hall, London, 1987) p. 191.Google Scholar
- 11.J. J. Bikerman, “The Science of Adhesive Joints” (Academic Press, New York, 1968) pp. 242–63.Google Scholar
- 12.K.-S. Kim, “Adhesion in Solids”, Vol. 119, edited by D. M. Mattox, J. E. E. Baglin, R. J. Gottschall and C. D. Batich (Materials Research Society, PA, 1988) pp. 31–41.Google Scholar
- 13.A. J. Kinloch,J. Mater. Sci. 17 (1982) 617.Google Scholar
- 14.
Copyright information
© Chapman & Hall 1992