Orientation of poly(ethylene terephthalate) in high-speed spinning using a heating zone
Chemistry and Technology of Chemical Fibres
Abstract
Data on high-speed spinning using a heating zone were analyzed. It was shown that in spinning at a speed of 3500–4000 m/min using a heating zone, it is possible to attain high orientation corresponding to the level of ultrahigh-speed spinning at 7000 m/min.
Keywords
Polymer Ethylene Terephthalate High Orientation Ethylene Terephthalate
These keywords were added by machine and not by the authors. This process is experimental and the keywords may be updated as the learning algorithm improves.
Preview
Unable to display preview. Download preview PDF.
References
- 1.Kh. Lukkert and U. Kemp, Khim. Volokna, No. 4, 48–52 (1994); Barmag Informations-Servise. No. 31. 11 (1991).Google Scholar
- 2.V. E. Geller, N. K. Zhiganov, and S. A. Gribanov, in: International Symposium on Chemical Fibres. Preprints [in Russian], Vol. 2, Kalinin (1990), p. 24.Google Scholar
- 3.V. E. Geller and L. A. Nikitina, Khim. Volokna No. 6, 37–38 (1993)Google Scholar
- 4.V. E. Geller, B. N. Averkiev, and E. M. Aizenshtein. Theoretical and Technological Aspects of High-Speed Spinning of Polyester Yarns [in Russian]. Data Sheet. Chemical Fibre Industry Series. NIITEKhim Moscow (1987), pp. 3, 11. 15.Google Scholar
- 5.V. E. Geller, Khim. Volokna, No. 3, 3–10 (1955).Google Scholar
Copyright information
© Plenum Publishing Corporation 1997