Skip to main content
Log in

An Evaluation of Moisture Damage Resistance of Asphalt Concrete based on Dynamic Creep Characteristics

  • Highway Engineering
  • Published:
KSCE Journal of Civil Engineering Aims and scope

Abstract

The performance of asphalt concrete is severely influenced by moisture. The presence of moisture in asphalt pavement substantially reduces its designed service lifetime. Currently, the indirect tensile strength test with constant loading rate is employed to estimate the moisture damage potential to an asphalt mixture. This evaluation method is empirical in nature and, therefore, suitable for only empirically designed asphalt pavements. However, speculation exists in that the conventional testing method may inappropriately simulate actual field conditions. Therefore, this research aims to evaluate the moisture damage potential to asphalt concrete under cyclic loading using the dynamic creep testing platform. The dynamic creep test provides the flow number, which represents the number of loading cycles at the failure point of the asphalt mixture. Three different types of asphalt mixtures commonly used in Western Australia were investigated in this research. The dynamic creep test provided more reasonable evaluation results of potential moisture damage than the conventional method. The tensile strength ratio of all mixtures in this research were greater than 80%, which is the conventional design criteria. On the other hand, the dynamic creep test reveals that flow number ratio of two mixtures dropped below 80%. The flow number ratio of 14 mm mixture was 58%, while 56% was obtained from 20 mm mixture. However, high uncertainty in the dynamic creep test results was observed, due to the interpretation technique. In conclusion, based on the research findings, the dynamic creep test can be used as a complementary test of the stripping potential in asphalt concrete.

This is a preview of subscription content, log in via an institution to check access.

Access this article

Price excludes VAT (USA)
Tax calculation will be finalised during checkout.

Instant access to the full article PDF.

Similar content being viewed by others

References

  • Al-Khateeb, G. and Basheer, I. (2009). “A three-stage rutting model utilising rutting performance data from the Humburg Wheel-Tracking Device (WTD).” Road and Transport Research: A Journal of Australian and New Zealand Research and Practice, Vol. 18, No. 3, pp. 12–25.

    Google Scholar 

  • Australian Asphalt Pavement Association (2005). Asphalt moisture sensitivity, Advisory Note 19, Australian Asphalt Pavement Association (AAPA), Melbourne, VIC, Australia.

  • Austroads (2007). Stripping potential of asphalt: Tensile strength ratio, AGPT/T232, Austroads, Sydney, NSW, Australia.

  • Austroads (2008). Testing asphalt in accordance with the Austroads mix design procedures, AP-T100/08, Austroads, Sydney, NSW, Australia.

  • Austroads (2017). Guide to pavement technology part 4F: Bituminous binders, AGPT04F-17, Austroads, Sydney, NSW, Australia.

  • Baghaee, M. T., Soltani, M., and Karim, M. R. (2014). “Evaluation of permanent deformation characteristics of unmodified and Polyethylene Terephthalate modified asphalt mixtures using dynamic creep test.” Materials & Design, Vol. 53, pp. 317–324, DOI: https://doi.org/10.1016/j.matdes.2013.07.015.

    Article  Google Scholar 

  • Beercroft, A., Petho, L., Griffin, J., and Denneman, E. (2014). “Asphalt moisture-sensitivity assessment in Australia using the Hamburg wheel tracking device.” 26th ARRB Conference, Sydney, NSW, Australia.

    Google Scholar 

  • Breakah, T. M. and Williams, R. C. (2013). “Dynamic testing of hot mix asphalt for moisture susceptibility assessment.” Construction and Building Materials, Vol. 47, pp. 636–642, DOI: https://doi.org/10.1016/j.conbuildmat.2013.05.014.

    Article  Google Scholar 

  • Cheng, D. X., Little, D. N., Lytton, R. L., and Holste, J. (2003). “Moisture damage evaluation of asphalt mixtures by considering both moisture diffusion and repeated-load conditions.” Transportation Research Record: Journal of the Transportation Research Board, Vol. 1832, pp. 32–49, DOI: https://doi.org/10.3141/1832-06.

    Article  Google Scholar 

  • Dehnad, M. H., Khodaii, A., and Moghadas Nejad, F. (2013). “Moisture sensitivity of asphalt mixtures under different load frequencies and temperatures.” Construction and Building Materials, Vol. 48, pp. 700–707, DOI: https://doi.org/10.1016/j.conbuildmat.2013.07.059.

    Article  Google Scholar 

  • Diab, A., Singh, D., and Pais, J. C. (2017). “Moisture susceptibility of asphlt mixtures: A literature review.” 4th Conference of Transportation Research Group of India (CTRG), Mumbai, India.

    Google Scholar 

  • Huang, B., Shu, X., Dong, Q., and Shen, J. (2017). “Laboratory evaluation of moisture susceptibility of hot-mix asphalt containing cementitious fillers.” Journal of Materials in Civil Engineering, ASCE, Vol. 22, No. 7, pp. 667–673, DOI: https://doi.org/10.1061/(ASCE)MT.1943-5533.0000064.

    Article  Google Scholar 

  • Kakar, M. R., Hamzah, M. O., and Valentin, J. (2015). “A review on moisture damages of hot and warm mix asphalt and related investigations.” Journal of Cleaner Production, Vol. 99, pp. 35–58, DOI: https://doi.org/10.1016/j.jclepro.2015.03.028.

    Article  Google Scholar 

  • Kandhal, S. P. and Chakaraborty, S. (1996). “Effect of Asphalt film thickness on short and long term aging of Asphalt paving mixtures.” Transportation Research Record: Journal of the Transportation Research Board, Vol. 1535, pp. 83–90, DOI: https://doi.org/10.3141/1535-11.

    Article  Google Scholar 

  • Kanitpong, K., Charoentham, N., and Likitlersuang, S. (2012). “Investigation on the effects of gradation and aggregate type to moisture damage of warm mix asphalt modified with Sasobit.” International Journal of Pavement Engineering, Vol. 13, No. 5, pp. 451–458, DOI: https://doi.org/10.1080/10298436.2011.565058.

    Article  Google Scholar 

  • Kim, S. and Brian, J. C. (2005). Evaluation of hot mix asphalt moisture sensitivity using the Nottingham asphalt test equipment, Final Report, Center for Transportation Research and Education, Iowa State University, Ames, IA, USA.

    Google Scholar 

  • Kumar, H. (2015). Dynamic creep test to predict moisture damage potential in an asphalt concrete mixture, BS Thesis, Curtin University, Perth, WA, Australia.

    Google Scholar 

  • Main Roads Western Australia (2011). Asphalt mix design, TRIM D11#103379, Main Roads Western Australia (MRWA), Perth, WA, Australia.

  • Main Roads Western Australia (2013). Engineering Road Note 9: Procedure for the design of road pavements, TRIM 05/5236, Main roads Western Australia (MRWA), Perth, WA, Australia.

  • Main Roads Western Australia (2015a). Specification 504: Asphalt wearing course, Main Roads Western Australia (MRWA), Perth, WA, Australia.

  • Main Roads Western Australia (2015b). Specification 510: Asphalt intermediate course, Main Roads Western Australia (MRWA), Perth, WA, Australia.

  • Mehrara, A. and Khodaii, A. (2011). “Evaluation of asphalt mixtures’ moisture sensitivity by dynamic creep test.” Journal of Materials in Civil Engineering, Vol. 23, No. 2, pp. 212–219, DOI: https://doi.org/10.1061/(ASCE)MT.1943-5533.0000146.

    Article  Google Scholar 

  • Mohamed, E. H. H., Abd El Halim, A. O., and Kennepohl, G. J. (1993). “Assessment of the influence of compaction method on asphalt concrete resistance to moisture damage.” Construction and Building Materials, Vol. 7, No. 3, pp. 149–156, DOI: https://doi.org/10.1016/0950-0618(93)90052-E.

    Article  Google Scholar 

  • Park, D. W., Seo, W. J., Kim, J., and Vo, H. V. (2017). “Evaluation of moisture susceptibility of asphalt mixture using liquid anti-stripping agents.” Construction and Building Materials, Vol. 144, pp. 399–405, DOI: https://doi.org/10.1016/j.conbuildmat.2017.03.214.

    Article  Google Scholar 

  • Sengoz, B. and Agar, E. (2007). “Effect of asphalt film thickness on the moisture sensitivity characteristics of hot-mix asphalt.” Building and Environment, Vol. 42, No. 10, pp. 3621–3628, DOI: https://doi.org/10.1016/j.buildenv.2006.10.006.

    Article  Google Scholar 

  • Standards Australia (1995). Methods of sampling and testing asphalt–Method 12.1: Determination of the permanent compressive strain characteristics of asphalt - Dynamic creep test, AS 2891.12.1, Standards Australia, Sydney, NSW, Australia.

  • Standards Australia (2014). Methods of sampling and testing asphalt–Method 2.2: Sample preparation - Compaction of asphalt test specimens using a gyratory compactor, AS 2891.2.2, Standards Australia, Sydney, NSW, Australia.

  • Terrel, R. L. and Al-sawailmi, S. (1994). Water sensitivity of asphaltaggregate mixes: Test selection, SHRP-A-403, Strategic Highway Research Program, National Research Council, Washington, DC, USA.

    Google Scholar 

Download references

Author information

Authors and Affiliations

Authors

Corresponding author

Correspondence to Korakod Nusit.

Rights and permissions

Reprints and permissions

About this article

Check for updates. Verify currency and authenticity via CrossMark

Cite this article

Jitsangiam, P., Nusit, K. & Nikraz, H. An Evaluation of Moisture Damage Resistance of Asphalt Concrete based on Dynamic Creep Characteristics. KSCE J Civ Eng 23, 1610–1616 (2019). https://doi.org/10.1007/s12205-019-1369-3

Download citation

  • Received:

  • Revised:

  • Accepted:

  • Published:

  • Issue Date:

  • DOI: https://doi.org/10.1007/s12205-019-1369-3

Keywords

Navigation