Heterogeneous Fenton degradation of Orange II by immobilization of Fe3O4 nanoparticles onto Al-Fe pillared bentonite

  • Catalysis, Reaction Engineering
  • Published:
Korean Journal of Chemical Engineering Aims and scope Submit manuscript

Abstract

A novel catalyst, Fe3O4 nanoparticle decorated Al-Fe pillared bentonite (Fe3O4/Al-Fe-P-B), was prepared by in situ precipitation oxidization method. The catalyst was characterized by SEM, XRD and Raman spectroscopy. The Fe3O4 nanoparticles mainly exist on the surface or enter into the pore of bentonite, with better dispersing and less coaggregation. The catalytic activity of Fe3O4/Al-Fe-P-B was investigated in the degradation of Orange II (OII) by heterogeneous Fenton-like process. The effects of initial concentration of hydrogen peroxide, catalyst loading, temperature and initial pH on the degradation of OII were investigated. The Fe3O4/Al-Fe-P-B showed higher degradation efficiency of OII than bare Fe3O4 or Al-Fe-P-B in the degradation experiment. The enhanced catalytic activity of Fe3O4/Al-Fe-P-B in heterogeneous Fenton system was due to the synergistic effect between Al-Fe-P-B and Fe3O4. The novel catalyst can achieve solid-liquid separation easily by sample magnetic separation and has a good reusability and stability.

This is a preview of subscription content, log in via an institution to check access.

Access this article

Price excludes VAT (USA)
Tax calculation will be finalised during checkout.

Instant access to the full article PDF.

Similar content being viewed by others

References

  1. K. Dutta, S. Mukhopadhyay, S. Bhattacharjee and B. Chaudhuri, J. Hazard. Mater., B 84, 57 (2001).

    Article  CAS  Google Scholar 

  2. G. Pliego, J. A. Zazo, J. A. Casas and J. J. Rodriguez, J. Hazard. Mater., 252-253, 180 (2013).

    Article  CAS  Google Scholar 

  3. L. Xu and J. Wang, J. Hazard. Mater., 186, 256 (2011).

    Article  CAS  Google Scholar 

  4. J. Feng, X. Hu and P. L. Yue, Environ. Sci. Technol., 38, 269 (2004).

    Article  CAS  Google Scholar 

  5. R. Matta, K. Hanna and S. Chiron, Sci. Total Environ., 385, 242 (2007).

    Article  CAS  Google Scholar 

  6. L. Gao, J. Zhuang, L. Nie, J. Zhang, Y. Zhang, N. Gu, T. Wang, J. Feng, D. Yang, S. Perrett and X. Yan, Nat. Nanotechnol., 2, 577 (2007).

    Article  CAS  Google Scholar 

  7. J. Zhang, J. Zhuang, L. Gao, Y. Zhang, N. Gu, J. Feng, D. Yang, J. Zhu and X. Yan, Chemosphere, 73, 1524 (2008).

    Article  CAS  Google Scholar 

  8. S. Zhang, X. Zhao, H. Niu, Y. Shi, Y. Cai and G. Jiang, J. Hazard. Mater., 167, 560 (2009).

    Article  CAS  Google Scholar 

  9. L. Xu and J. Wang, Appl. Catal. B: Environ., 123-124, 117 (2012).

    Article  CAS  Google Scholar 

  10. S. P. Sun and A. T. Lemley, J. Mol. Catal. A-Chem., 349, 71 (2011).

    Article  CAS  Google Scholar 

  11. N. Wang, L. Zhu, M. Wang, D. Wang and H. Tang, Ultrason. Sonochem., 17, 78 (2010).

    Article  CAS  Google Scholar 

  12. N. Wang, L. Zhu, D. Wang, M. Wang, Z. Lin and H. Tang, Ultrason. Sonochem., 17, 526 (2010).

    Article  CAS  Google Scholar 

  13. M. H. Do, N. H. Phan, T. D. Nguyen, T. T. S. Pham, V. K. Nguyen, T. T. T. Vu and T. K. P. Nguyen, Chemosphere, 85, 1269 (2011).

    Article  CAS  Google Scholar 

  14. X. Hu, B. Liu, Y. Deng, H. Chen, S. Luo, C. Sun, P. Yang and S. Yang, Appl. Catal. B: Environ., 107, 274 (2011).

    Article  CAS  Google Scholar 

  15. J. Chun, H. Lee, S. H. Lee, S. W. Hong, J. Lee, C. Lee and J. Lee, Chemosphere, 89, 1230 (2012).

    Article  CAS  Google Scholar 

  16. S. Shin, H. Yoon and J. Jang, Cataly. Commun., 10, 178 (2008).

    Article  CAS  Google Scholar 

  17. Y. S. Shin, S. G. Oh and B. H. Ha, Korean J. Chem. Eng., 20, 77 (2003).

    Article  CAS  Google Scholar 

  18. S. Mnasri-Ghnimi and N. Frini-Srasra, Korean J. Chem. Eng., 32, 68 (2015).

    Article  CAS  Google Scholar 

  19. N. Ksontini, W. Najjar and A. Ghorbel, J. Phys. Chem. Solids, 69, 1112 (2008).

    Article  CAS  Google Scholar 

  20. M. Luo, D. Bowden and P. Brimblecombe, Appl. Catal. B: Environ., 85, 201 (2009).

    Article  CAS  Google Scholar 

  21. D. Wan, G. H. Wang, W. B. Li, K. Chen and G. Shu, Acta Phys. - Chim. Sin., 29, 2429 (2013).

    CAS  Google Scholar 

  22. L. C. A. Oliveira, R. V. R. A. Rios, J. D. Fabris, K. Sapag, V. K. Garg and R. M. Lago, Appl. Clay Sci., 22, 169 (2003).

    Article  CAS  Google Scholar 

  23. P. Yuan, M. Fan, D. Yang, H. He, D. Liu, A. Yuan, J. Zhu and T. Chen, J. Hazard. Mater., 166, 821 (2009).

    Article  CAS  Google Scholar 

  24. S. Hashemian and H. Saffari, Asian J. Chem., 23, 2815 (2011).

    CAS  Google Scholar 

  25. I. Larraza, M. López-Gónzalez, T. Corrales and G. Marcelo, J. Colloid Interf. Sci., 385, 24 (2012).

    Article  CAS  Google Scholar 

  26. L. Lian, X. Cao, Y. Wu, D. Sun and D. Lou, Appl. Surf. Sci., 289, 245 (2014).

    Article  CAS  Google Scholar 

  27. G. H. Wang, Y. Z. Lu, W. B. Li, X. Q. Liu and M. D. Sun, Adv. Mater. Res., 581-582, 292 (2012).

    Article  CAS  Google Scholar 

  28. X. Xue, K. Hanna and N. Deng, J. Hazard. Mater., 166, 407 (2009).

    Article  CAS  Google Scholar 

  29. L. Chen, C. Deng, F. Wu and N. Deng, Desalination, 281, 306 (2011).

    Article  CAS  Google Scholar 

  30. M. Neamtu, C. Zaharia, C. Catrinescu, A. Yediler, M. Macoveanu and A. Kettrup, Appl. Catal. B: Environ., 48, 287 (2004).

    Article  CAS  Google Scholar 

  31. Y. Liu, W. Jiang, Y. Wang, X. J. Zhang, D. Song and F. S. Li, J. Magn. Magn. Mater., 321, 408 (2009).

    Article  CAS  Google Scholar 

  32. R. L. Frost and L. Rintoul, Appl. Clay Sci., 11, 171 (1996).

    Article  CAS  Google Scholar 

  33. S. Tiwari, D. M. Phase and R. J. Choudhary, Appl. Phys. Lett., 93, (2008).

    Google Scholar 

  34. X. Liang, Y. Zhong, S. Zhu, J. Zhu, P. Yuan, H. He and J. Zhang, J. Hazard. Mater., 181, 112 (2010).

    Article  CAS  Google Scholar 

  35. J. H. Ramirez, F. J. Maldonado-Hódar, A. F. Pérez-Cadenas, C. Moreno-Castilla, C. A. Costa and L. M. Madeira, Appl. Catal. B: Environ., 75, 312 (2007).

    Article  CAS  Google Scholar 

  36. J. H. Ramirez, C. A. Costa, L. M. Madeira, G. Mata, M. A. Vicente, M. L. Rojas-Cervantes, A. J. López-Peinado and R. M. Martín-Aranda, Appl. Catal. B: Environ., 71, 44 (2007).

    Article  CAS  Google Scholar 

  37. M. L. Rache, A. R. García, H. R. Zea, A. M. T. Silva, L. M. Madeira and J. H. Ramírez, Appl. Catal. B: Environ., 146, 192 (2014).

    Article  CAS  Google Scholar 

Download references

Author information

Authors and Affiliations

Authors

Corresponding authors

Correspondence to Wenbing Li or Dong Wan.

Electronic supplementary material

Rights and permissions

Reprints and permissions

About this article

Check for updates. Verify currency and authenticity via CrossMark

Cite this article

Li, W., Wan, D., Wang, G. et al. Heterogeneous Fenton degradation of Orange II by immobilization of Fe3O4 nanoparticles onto Al-Fe pillared bentonite. Korean J. Chem. Eng. 33, 1557–1564 (2016). https://doi.org/10.1007/s11814-016-0005-x

Download citation

  • Received:

  • Accepted:

  • Published:

  • Issue Date:

  • DOI: https://doi.org/10.1007/s11814-016-0005-x

Keywords

Navigation