Light scattering by boron oxide in the temperature range of 225–330°C

  • Published:
Glass Physics and Chemistry Aims and scope Submit manuscript

Abstract

It is found that the process of variation in the intensity of the polarized component of the light scattered by boron oxide in the temperature range of 250–290°C after cooling from temperatures of 330 and 450°C possesses the peculiarities similar to those found earlier for the step-by-step mode of cooling for temperatures higher than 295°C and is characterized by the formation of a minimum. It is also detected that at lower temperatures the minimum possesses an asymmetric shape. It is shown that the process of increasing the intensity in time is satisfactorily approximated by an empirical equation of an exponential form. It is found that the change in the relaxation times with the temperature corresponds to an exponential law for the entire set of the data that we have obtained. It is found that the change in the depolarized component intensity in the region of low temperatures is relatively small, which makes it possible to associate the behavior of the polarized component with the change in the value of isotropic scattering. It is shown that in agreement with the results obtained earlier the time dependence of the intensity of the polarized component at a higher temperature for a sample preliminarily annealed at a low temperature is characterized by the formation of a maximum. The experimental results that we have obtained indicate the universal character of the manifestation of a peculiarity in the behavior of the scattered light intensity in the process of cooling and heating of boron oxide in the glass transition range.

This is a preview of subscription content, log in via an institution to check access.

Access this article

Price excludes VAT (USA)
Tax calculation will be finalised during checkout.

Instant access to the full article PDF.

Similar content being viewed by others

References

  1. Bokov, N.A., Universal character of light scattering intensity relaxation by boron oxyde melt in temperate range 300–340°C, Fiz. Khim. Stekla, 2016, vol. 42, no. 6 (in press).

    Google Scholar 

  2. Bokov, N.A., The light scattering studies of glasses in the glass transition region, J. Non-Cryst. Solids, 1994, vol. 177, nos. 1–2, pp. 74–80.

    Article  Google Scholar 

  3. Bokov, N.A., Peculiarities of structure relaxation of boric oxide in the glass transition region according to the light scattering data, Glass Phys. Chem., 2015, vol. 41, no. 1, pp. 31–34.

    Article  Google Scholar 

  4. Bokov, N.A., Ultraslow relaxation process of static light scattering intensity by boron oxide above the glass transition temperature, J. Mater. Sci. Chem. Eng., 2015, vol. 3, no. 7, pp. 75–80.

    Google Scholar 

  5. Bokov, N.A., Peculiarities of light scattering by boron oxide glass, Glass Phys. Chem., 2016, vol. 42, no. 4, pp. 386–392.

    Article  Google Scholar 

  6. Golubkov, V.V., Relaxation of structure in the glass transition region of B2O3, Fiz. Khim. Stekla, 1989, vol. 15, no. 3, pp. 467–479.

    Google Scholar 

  7. Macedo, P.B., Montrose, C.J., Moynihan, C.T., and Lai, C.C., Viscoelastic relaxation in B2O3, in Proceedings of the Conference of Boron Glass and Glass Ceramics, New York: Alfred, 1977; New York: Plenum, 1978, pp. 463–476.

    Google Scholar 

  8. Moynihan, C.T. and Schroeder, J., Non-exponential structural relaxation, anomalous light scattering and nanoscale inhomogeneities in glass-forming liquids, J. Non-Cryst. Solids, 1993, vol. 160, nos. 1–2, pp. 52–59.

    Article  Google Scholar 

Download references

Author information

Authors and Affiliations

Authors

Corresponding author

Correspondence to N. A. Bokov.

Additional information

Original Russian Text © N.A. Bokov, 2017, published in Fizika i Khimiya Stekla.

Rights and permissions

Reprints and permissions

About this article

Check for updates. Verify currency and authenticity via CrossMark

Cite this article

Bokov, N.A. Light scattering by boron oxide in the temperature range of 225–330°C. Glass Phys Chem 43, 17–22 (2017). https://doi.org/10.1134/S1087659617010047

Download citation

  • Received:

  • Published:

  • Issue Date:

  • DOI: https://doi.org/10.1134/S1087659617010047

Keywords

Navigation