, Volume 51, Issue 5, pp 357-363

Prehydrolysis ofEucalyptus wood with dilute sulphuric acid: operation at atmospheric pressure

Rent the article at a discount

Rent now

* Final gross prices may vary according to local VAT.

Get Access

Abstract

MilledEucalyptus globulus wood samples were subjected to acid hydrolysis using H2SO4 as catalyst. The reactions were carried out in a stirred, reflux-operated batch reactor. The effects of both catalyst concentration (in the range 3.5–10%) and hydrolysis time (0–11 h) on the concentration of arabinose, glucose, xylose, acetic acid and furfural were studied. The kinetics of xylan hydrolysis followed general trends similar to those described in earlier studies. Almost quantitative xylose recovery was achieved after 11 h of reaction time in experiments with 10% H2SO4. The furfural concentrations were low (0–0.44 g/L) in all the cases studied. Additional aspects relative to the selectivity of the prehydrolysis are discussed.

Zusammenfassung

Gemahlenes Holz vonEucalyptus globulus wurde mit verdünnter Schwefelsäure als Katalysator behandelt. Die Reaktion erfolgte unter Rühren und Rückfluß. Untersucht wurde der Einfluß der Katalysatorkonzentration (3.5–10%) und der Reaktionszeit (0–11 h) auf die Ausbeute der Reaktionsprodukte Arabinose, Glucose, Xylose, Essigsäure und Furfural. Die Kinetik der Xylan-Hydrolyse entsprach den Ergebnissen früherer Untersuchungen. Eine nahezu 100%ige Xylose-Ausbeute wurde nach 11 h mit 10%iger H2SO4 erreicht. Die Furfural-Konzentration war in allen Experimenten niedrig (0–0,44 g/L). Weiterhin werden Aspekte einer selektiven Vorhydrolyse diskutiert.