Preparation and properties of new polyamides from 1,6-diaminodiamantane and aromatic diacid chlorides

  • Yaw-Terng Chern
  • Ming-Cherng Lin
Article

DOI: 10.1007/BF00312892

Cite this article as:
Chern, YT. & Lin, MC. Polymer Bulletin (1995) 35: 41. doi:10.1007/BF00312892

Summary

New polyamides were prepared by the solution polycondensation and interfacial polycondensation starting from 1,6-diaminodiamantane and aromatic diacid chlorides. The polyamides had inherent viscosities of 0.15–0.45 dL/g. The temperatures at 5% weight loss for the polyamides were between 435–475°C in nitrogen. The glass transition temperatures of the polyamides determined by DSC ranged from 245°C to 300°C. The crystallinity of the resultant polyamides was influenced by the method of polycondensation and various monomers.

Copyright information

© Springer-Verlag 1995

Authors and Affiliations

  • Yaw-Terng Chern
    • 1
  • Ming-Cherng Lin
    • 1
  1. 1.Institute of Chemical EngineeringNational Taiwan Institute of TechnologyTaipeiTaiwan, Republic of China